Joon-Oh MOON has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Publication number: 20240086712
    Abstract: Provided are a method for evaluating performance and a system thereof. The method according to some embodiments may include obtaining a first model trained using a labeled dataset, obtaining a second model built by performing unsupervised domain adaptation on the first model, generating pseudo labels for an evaluation dataset using the second model, wherein the evaluation dataset is an unlabeled dataset, and evaluating performance of the first model using the pseudo labels.
    Type: Application
    Filed: June 23, 2023
    Publication date: March 14, 2024
    Applicant: SAMSUNG SDS CO., LTD.
    Inventors: Joon Ho LEE, Han Kyu Moon, Jae Oh Woo
  • Patent number: 10480053
    Abstract: The present invention relates to an austenitic light-weight high-strength steel with excellent properties of welds, and a method of manufacturing the same, the method including: (a) hot-rolling a steel including 20 wt % to 30 wt % of manganese (Mn), 6 wt % to 12 wt % of aluminum (Al), 0.6 wt % to 1.5 wt % of carbon (C), 0.3 wt % to 0.95 wt % of vanadium (V), and a remaining amount of iron (Fe) and other unavoidable impurities; (b) homogenizing the hot-rolled steel; and (c) aging the homogenized steel.
    Type: Grant
    Filed: November 24, 2015
    Date of Patent: November 19, 2019
    Assignee: KOREA INSTITUTE OF MACHINERY AND MATERIALS
    Inventors: Joon-Oh Moon, Seong-Jun Park, Chang-Hoon Lee
  • Publication number: 20160153077
    Abstract: The present invention relates to an austenitic light-weight high-strength steel with excellent properties of welds, and a method of manufacturing the same, the method including: (a) hot-rolling a steel including 20 wt % to 30 wt % of manganese (Mn), 6 wt % to 12 wt % of aluminum (Al), 0.6 wt % to 1.5 wt % of carbon (C), 0.3 wt % to 0.95 wt % of vanadium (V), and a remaining amount of iron (Fe) and other unavoidable impurities; (b) homogenizing the hot-rolled steel; and (c) aging the homogenized steel.
    Type: Application
    Filed: November 24, 2015
    Publication date: June 2, 2016
    Inventors: Joon-Oh MOON, Seong-Jun PARK, Chang-Hoon LEE