  • Patent number: 11485815
    Abstract: A 4-methyl-1-pentene polymer particle (X) which satisfies the following requirements (X-a), (X-b) and (X-c): (X-a) being composed of a 4-methyl-1-pentene polymer which has a content of a constitutional unit derived from 4-methyl-1-pentene being 30.0 to 99.7% by mol, and a content of a constitutional unit derived from at least one olefin selected from ethylene and an ?-olefin having 3 to 20 carbon atoms (except for 4-methyl-1-pentene) being 0.3 to 70.0% by mol; (X-b) having, when measured in a cross fractionation chromatograph apparatus (CFC) using an infrared spectrophotometer as a detector part, at least one peak A of an amount of a component eluted present in the range of 100 to 140° C., and at least one peak B of an amount of a component eluted present at lower than 100° C.; and (X-c) having a meso diad fraction (m) measured by 13C-NMR falling within the range of 95.0 to 100%.
    Type: Grant
    Filed: April 9, 2019
    Date of Patent: November 1, 2022
    Assignee: MITSUI CHEMICALS, INC.
    Inventors: Masakazu Tanaka, Toyoaki Sasaki, Tomoaki Matsugi, Sadahiko Matsuura, Naoto Matsukawa, Masatoshi Chinaka
  • Publication number: 20210032397
    Abstract: A 4-methyl-1-pentene polymer particle (X) which satisfies the following requirements (X-a), (X-b) and (X-c): (X-a) being composed of a 4-methyl-1-pentene polymer which has a content of a constitutional unit derived from 4-methyl-1-pentene being 30.0 to 99.7% by mol, and a content of a constitutional unit derived from at least one olefin selected from ethylene and an ?-olefin having 3 to 20 carbon atoms (except for 4-methyl-1-pentene) being 0.3 to 70.0% by mol; (X-b) having, when measured in a cross fractionation chromatograph apparatus (CFC) using an infrared spectrophotometer as a detector part, at least one peak A of an amount of a component eluted present in the range of 100 to 140° C., and at least one peak B of an amount of a component eluted present at lower than 100° C.; and (X-c) having a meso diad fraction (m) measured by 13C-NMR falling within the range of 95.0 to 100%.
    Type: Application
    Filed: April 9, 2019
    Publication date: February 4, 2021
    Applicant: MITSUI CHEMICALS, INC.
    Inventors: Masakazu TANAKA, Toyoaki SASAKI, Tomoaki MATSUGI, Sadahiko MATSUURA, Naoto MATSUKAWA, Masatoshi CHINAKA
  • Patent number: 8445609
    Abstract: An object of the present invention is to provide a method for producing an olefin polymer, with which an olefin polymer having good particle properties can be produced in high activity, fouling inside the polymerization vessel, such as a vessel wall or an impeller, can be effectively prevented, and a long-term stable operation is achieved. A method for producing an olefin polymer according to the present invention is characterized by including (co)polymerizing at least one olefin selected from the group consisting of ethylene and ?-olefins having 3 to 20 carbon atoms in a polymerization vessel in the presence of (A) a solid catalyst component for olefin polymerization, (B) an aliphatic amide, and (C) an organoaluminum compound.
    Type: Grant
    Filed: April 21, 2010
    Date of Patent: May 21, 2013
    Assignees: Mitsui Chemicals, Inc., Prime Polymer Co., Ltd.
    Inventors: Yasushi Tohi, Ken Yoshitsugu, Naoya Akiyama, Toshio Fujita, Masatoshi Chinaka
  • Publication number: 20120041162
    Abstract: [Object] An object of the present invention is to provide a method for producing an olefin polymer, with which an olefin polymer having good particle properties can be produced in high activity, contamination inside the polymerization vessel, such as a vessel wall or an impeller, can be effectively prevented, and a long-term stable operation is achieved. [Means for Achieving the Object] A method for producing an olefin polymer according to the present invention is characterized by including (co)polymerizing at least one olefin selected from the group consisting of ethylene and ?-olefins having 3 to 20 carbon atoms in a polymerization vessel in the presence of (A) a solid catalyst component for olefin polymerization, (B) an aliphatic amide, and (C) an organoaluminum compound.
    Type: Application
    Filed: April 21, 2010
    Publication date: February 16, 2012