  • Patent number: 12191060
    Abstract: Provided a soft magnetic alloy ribbon containing Fe and B. Convex portions having an average convex portion height of 7 nm to 130 nm are present on an alloy surface.
    Type: Grant
    Filed: August 23, 2022
    Date of Patent: January 7, 2025
    Assignee: TDK CORPORATION
    Inventors: Kyotaro Abe, Isao Nakahata, Takuya Tsukahara
  • Patent number: 12159743
    Abstract: The object of the present invention is to provide an alloy ribbon capable of having excellent adhesiveness between the alloy ribbons when a plurality of the alloy ribbons is stacked; and also, to provide a magnetic core using the alloy ribbon. The present invention is an alloy ribbon comprising metals scattered on at least one surface of the alloy ribbon, in which diameters of the scattered metals are 1 ?m or more, and the scattered metals include Cu.
    Type: Grant
    Filed: March 23, 2021
    Date of Patent: December 3, 2024
    Assignee: TDK CORPORATION
    Inventors: Kyotaro Abe, Takuya Tsukahara, Isao Nakahata, Kazuhiro Yoshidome
  • Patent number: 12062475
    Abstract: To provide a soft magnetic alloy or the like, from which a magnetic component having a good temperature property of core loss can be obtained. The soft magnetic alloy includes Fe. The soft magnetic alloy includes a crystallite, and an amorphous phase existing around the crystallite. A total area ratio of the crystallite in a cross section of the soft magnetic alloy is 40% or more and less than 60%. An average thickness of the amorphous phase is 3.0 nm or more and 10.0 nm or less. A standard deviation of a thickness of the amorphous phase is 10.0 nm or less.
    Type: Grant
    Filed: March 24, 2022
    Date of Patent: August 13, 2024
    Assignee: TDK CORPORATION
    Inventors: Takuya Tsukahara, Isao Nakahata, Kazuhiro Yoshidome
  • Patent number: 11955261
    Abstract: A specific depth at which a concentration of Fe reaches 10 at % is 18 nm or more and 500 nm or less from the first surface, and from the first surface to the specific depth, the concentration of Fe is less than 10 at %, and a positive increase region is present in which the concentration of Fe increases with a substantially positive concentration gradient, in a case where the concentration of Fe is measured in a depth direction from a first surface of a ribbon.
    Type: Grant
    Filed: August 23, 2022
    Date of Patent: April 9, 2024
    Assignee: TDK CORPORATION
    Inventors: Kyotaro Abe, Isao Nakahata, Takuya Tsukahara
  • Publication number: 20230149482
    Abstract: An object of one present invention is to provide a food composition including, as an active ingredient thereof, Lactobacillus mucosae that has a function of improving a gut microbiota. An object of another present invention is to provide an increasing drug for the rate of bifidobacteria in the human intestine and a bifidobacteria proliferation promoting drug, including Lactobacillus mucosae as an active ingredient thereof. The one present invention provides a composition for improving the gut microbiota, including the bacterial cell or a culture of Lactobacillus mucosae as an active ingredient thereof. The other present invention provides an increasing drug for the rate of bifidobacteria in the human intestine and a bifidobacteria proliferation promoting drug, including Lactobacillus mucosae as an active ingredient thereof.
    Type: Application
    Filed: April 7, 2021
    Publication date: May 18, 2023
    Applicant: MEGMILK SNOW BRAND CO., LTD.
    Inventors: Shigeki KADA, Takuya TSUKAHARA, Akira KIMURA, Nana OGAWA
  • Publication number: 20230079841
    Abstract: Provided a soft magnetic alloy ribbon containing Fe and B. Convex portions having an average convex portion height of 7 nm to 130 nm are present on an alloy surface.
    Type: Application
    Filed: August 23, 2022
    Publication date: March 16, 2023
    Applicant: TDK CORPORATION
    Inventors: Kyotaro ABE, Isao NAKAHATA, Takuya TSUKAHARA
  • Publication number: 20230085009
    Abstract: A specific depth at which a concentration of Fe reaches 10 at % is 18 nm or more and 500 nm or less from the first surface, and from the first surface to the specific depth, the concentration of Fe is less than 10 at %, and a positive increase region is present in which the concentration of Fe increases with a substantially positive concentration gradient, in a case where the concentration of Fe is measured in a depth direction from a first surface of a ribbon.
    Type: Application
    Filed: August 23, 2022
    Publication date: March 16, 2023
    Applicant: TDK CORPORATION
    Inventors: Kyotaro ABE, Isao NAKAHATA, Takuya TSUKAHARA
  • Publication number: 20220328224
    Abstract: To provide a soft magnetic alloy or the like, from which a magnetic component having a good temperature property of core loss can be obtained. The soft magnetic alloy includes Fe. The soft magnetic alloy includes a crystallite, and an amorphous phase existing around the crystallite. A total area ratio of the crystallite in a cross section of the soft magnetic alloy is 40% or more and less than 60%. An average thickness of the amorphous phase is 3.0 nm or more and 10.0 nm or less. A standard deviation of a thickness of the amorphous phase is 10.0 nm or less.
    Type: Application
    Filed: March 24, 2022
    Publication date: October 13, 2022
    Applicant: TDK CORPORATION
    Inventors: Takuya TSUKAHARA, Isao NAKAHATA, Kazuhiro YOSHIDOME
  • Patent number: 11441213
    Abstract: A soft magnetic alloy ribbon having high corrosion resistance and good magnetic properties is obtained. The soft magnetic alloy ribbon contains Fe and M. M is at least one selected from the group consisting of Nb, Ta, W, Zr, Hf, Mo, Cr, and Ti, and a part of M is included in oxides. A maximum point of a concentration of at least one of M included in the oxides is present in a region within 20 nm from the surface, when a concentration distribution of an element contained in the soft magnetic alloy ribbon is measured from a surface toward an interior of the soft magnetic alloy ribbon in a thickness direction.
    Type: Grant
    Filed: November 19, 2020
    Date of Patent: September 13, 2022
    Assignee: TDK CORPORATION
    Inventors: Takuya Tsukahara, Isao Nakahata, Kazuhiro Yoshidome, Hiroyuki Matsumoto
  • Publication number: 20210301380
    Abstract: An alloy ribbon that is an alloy ribbon containing a metal as a main component, and has a recess on at least one principal surface, in which a depth of the recess is 5% or more and 75% or less of an average thickness.
    Type: Application
    Filed: March 25, 2021
    Publication date: September 30, 2021
    Applicant: TDK CORPORATION
    Inventors: Isao NAKAHATA, Takuya TSUKAHARA
  • Publication number: 20210304936
    Abstract: The object of the present invention is to provide an alloy ribbon capable of having excellent adhesiveness between the alloy ribbons when a plurality of the alloy ribbons is stacked; and also, to provide a magnetic core using the alloy ribbon. The present invention is an alloy ribbon comprising metals scattered on at least one surface of the alloy ribbon, in which diameters of the scattered metals are 1 ?m or more, and the scattered metals include Cu.
    Type: Application
    Filed: March 23, 2021
    Publication date: September 30, 2021
    Applicant: TDK CORPORATION
    Inventors: Kyotaro ABE, Takuya TSUKAHARA, Isao NAKAHATA, Kazuhiro YOSHIDOME
  • Publication number: 20210156011
    Abstract: A soft magnetic alloy ribbon having high corrosion resistance and good magnetic properties is obtained. The soft magnetic alloy ribbon contains Fe and M. M is at least one selected from the group consisting of Nb, Ta, W, Zr, Hf, Mo, Cr, and Ti, and a part of M is included in oxides. A maximum point of a concentration of at least one of M included in the oxides is present in a region within 20 nm from the surface, when a concentration distribution of an element contained in the soft magnetic alloy ribbon is measured from a surface toward an interior of the soft magnetic alloy ribbon in a thickness direction.
    Type: Application
    Filed: November 19, 2020
    Publication date: May 27, 2021
    Applicant: TDK CORPORATION
    Inventors: Takuya TSUKAHARA, Isao NAKAHATA, Kazuhiro YOSHIDOME, Hiroyuki MATSUMOTO
  • Publication number: 20210159001
    Abstract: A soft magnetic alloy ribbon having high corrosion resistance is obtained. The soft magnetic alloy ribbon contains Fe, P, and Si. A maximum point of a concentration of P and a maximum point of a concentration of Si including in oxides is present in a region within 20 nm from the surface, when a concentration distribution of an element contained in the soft magnetic alloy ribbon is measured from a surface toward an interior of the soft magnetic alloy ribbon in a thickness direction.
    Type: Application
    Filed: November 19, 2020
    Publication date: May 27, 2021
    Applicant: TDK CORPORATION
    Inventors: Takuya TSUKAHARA, Isao NAKAHATA, Kazuhiro YOSHIDOME, Hiroyuki MATSUMOTO