Abstract: In the manufacture of iron in which coke and coal are added to a blast furnace during iron manufacture, an improvement for enhancing the operation of the furnace is disclosed. A metallic element in the form of a compound thereof, the metallic element selected from zirconium, chromium, molybdenum, tungsten, manganese, iron, cobalt, nickel, copper, zinc, aluminum, tin and lead is added to the coal, allowing for a reduction in the amount of coke added to the furnace.
Type:
Grant
Filed:
June 9, 1998
Date of Patent:
June 20, 2000
Assignee:
BetzDearborn Inc.
Inventors:
Muthukumaraswamy Karanai Margan, Santanu Ghosh, Indronil Sengupta, James S. McNeill
Abstract: A method of ironmaking by means of a smelting shaft furnace including the steps of supplying iron ore and coke to the top of the furnace; and injecting coal and oxygen into the smelting zone of the furnace to promote combustion, to control reaction temperature and provide heat for smelting, the quantities of coal and oxygen injection being within the range of 0.7 to 1.7 of stoichiometric conditions with respect to combustion to carbon monoxide and hydrogen.