Abstract: Zeolite/clay/phosphate catalysts can be prepared by a process wherein a composition of zeolite-clay-phosphate is brought to a pH level of about 7.0 to about 14.0. The resulting slurry is then age reacted for about 0.5 to about 24 hours. Thereafter the slurry is dried to produce a zeolite/clay/phosphate catalyst particles that are particularly characterized by their high levels of zeolite stability.
Abstract: The useful life of SO.sub.X additives having a SO.sub.2 .fwdarw.SO.sub.3 oxidation catalyst component and a SO.sub.3 absorption component can be extended by employing each of these components as separate and distinct physical particles, pellets, etc.
Type:
Grant
Filed:
September 3, 1997
Date of Patent:
June 13, 2000
Assignee:
Bulldog Technologies U.S.A., Inc.
Inventors:
Edward J. Demmel, deceased, Albert A. Vierheilig, Regis B. Lippert
Abstract: The useful life of SO.sub.X additives having a SO.sub.2 .fwdarw.SO.sub.3 oxidation catalyst component and a SO.sub.3 absorption component can be extended by employing each of these components as separate and distinct physical particles, pellets, etc., with each component having large proportions of certain ingredients and having small proportions of certain other ingredients.
Type:
Grant
Filed:
November 18, 1996
Date of Patent:
April 11, 2000
Assignee:
Bulldog Technologies U.S.A., Inc.
Inventors:
Edward J. Demmel, Albert A. Vierheilig, Regis B. Lippert
Abstract: Anionic clay compounds such as hydrotalcite-like compounds can be made by a process wherein a non-hydrotalcite-like compound (or a hydrotalcite-like compound) are heat treated and then hydrated to form hydrotalcite-like compounds having properties (e.g., increased hardness and/or density) that differ from those of hydrotalcite-like compounds made by prior art methods wherein non-hydrotalcite-like compounds (or hydrotalcite-like compounds) are not similarly heat treated and hydrated to form such hydrotalcite-like compounds.
Abstract: Zeolite/clay/phosphate catalysts can be prepared by a process wherein a composition of zeolite-clay-phosphate is brought to a pH level of about 7.0 to about 14.0. The resulting slurry is then age reacted for about 0.5 to about 24 hours. Thereafter the slurry is dried to produce a zeolite/clay/phosphate catalyst particles that are particularly characterized by their high levels of zeolite stability.
Abstract: A valve for introducing particulate materials into a high pressure gas stream and for preventing said particulate materials from invading those interior regions of the valve having moving parts.