Abstract: A method for separating a calcite-rich low-grade fluorite barite paragenic ore, includes the following steps: S1, crushing; S2, performing classification on a crushed ore to obtain a fine-grained ore, a medium-grained ore and a coarse-grained ore; S3, performing jigging gravity separation on the medium-grained ore and the coarse-grained ore to obtain first barite concentrates and jigging tailings; S4, performing color sorting on the jigging tailings to obtain calcite minerals and color sorting tailings; S5, combining the fine-grained ore and the color sorting tailings, and then performing ore grinding to obtain feeding materials in flotation; S6, performing flotation on the feeding materials in flotation to obtain fluorite concentrates and flotation tailings; S7, performing chute gravity separation on the flotation tailings to obtain second barite concentrates and chute tailings. The method achieves an effect of obtaining high-quality acid-grade fluorite concentrates (CaF2?98%).
Type:
Grant
Filed:
January 26, 2021
Date of Patent:
October 25, 2022
Assignee:
INSTITUTE OF MULTIPURPOSE UTILIZATION OF MINERAL RESOURCES, CAGS
Abstract: A method for separating a calcite-rich low-grade fluorite barite paragenic ore, includes the following steps: S1, crushing; S2, performing classification on a crushed ore to obtain a fine-grained ore, a medium-grained ore and a coarse-grained ore; S3, performing jigging gravity separation on the medium-grained ore and the coarse-grained ore to obtain first barite concentrates and jigging tailings; S4, performing color sorting on the jigging tailings to obtain calcite minerals and color sorting tailings; S5, combining the fine-grained ore and the color sorting tailings, and then performing ore grinding to obtain feeding materials in flotation; S6, performing flotation on the feeding materials in flotation to obtain fluorite concentrates and flotation tailings; S7, performing chute gravity separation on the flotation tailings to obtain second barite concentrates and chute tailings. The method achieves an effect of obtaining high-quality acid-grade fluorite concentrates (CaF2?98%).
Type:
Application
Filed:
January 26, 2021
Publication date:
June 30, 2022
Applicant:
Institute of Multipurpose Utilization of Mineral Resources, CAGS
Abstract: An ore dressing process for medium-grade and low-grade mixed collophanite includes the following steps: S1; crushing ores to obtain crushed ores; S2: screening the crushed ores to obtain fine-fraction ores and coarse-fraction ores divided into at least two size fractions; S3: performing a photoelectric separation to the coarse-fraction ores of different size fractions to obtain photoelectric separation concentrates and photoelectric separation tailings of each size fraction; S4: combining the photoelectric separation concentrates of the each size fraction to obtain pre-enriched concentrates; S5: combining the fine-fraction ores and the pre-enriched concentrates, and then performing an ore grinding to obtain minerals to be separated; S6: adding water to the minerals to be separated to obtain a floatation pulp, and then performing a floatation to obtain phosphate concentrates and tailings.
Type:
Application
Filed:
February 4, 2021
Publication date:
June 16, 2022
Applicant:
Institute of Multipurpose Utilization of Mineral Resources, CAGS
Inventors: