Abstract: An oil type release agent is provided, containing 70 to 98 parts by weight of solvents having dynamic viscosity of 2 to 10 mm2/s at 40° C. and a flash point in the range of 70 to 170° C., 1 to 10 parts by weight of high viscosity mineral oils and/or synthetic oils having dynamic viscosity of 100 mm2/s or higher at 40° C., 15 parts by weight or less of a silicone oil having dynamic viscosity of 150 mm2/s or higher at 40° C., and 1 to 5 parts by weight of additives having a lubricating function. The flash point of the agent is in the range of 70 to 170° C., and the dynamic viscosity of the agent is 2 to 30 mm2/s or higher at 40° C.
Type:
Grant
Filed:
February 12, 2012
Date of Patent:
July 1, 2014
Assignees:
Aoki Science Institute Co., Ltd., Ryobi Ltd., Kotobuki Kinzoku Kogyo Co., Ltd., Aisan Industry Co., Ltd.
Abstract: An oil type release agent is provided, containing 70 to 98 parts by weight of solvents having dynamic viscosity of 2 to 10 mm2/s at 40° C. and a flash point in the range of 70 to 170° C., 1 to 10 parts by weight of high viscosity mineral oils and/or synthetic oils having dynamic viscosity of 100 mm2/s or higher at 40° C., 15 parts by weight or less of a silicone oil having dynamic viscosity of 150 mm2/s or higher at 40° C., and 1 to 5 parts by weight of additives having a lubricating function. The flash point of the agent is in the range of 70 to 170° C., and the dynamic viscosity of the agent is 2 to 30 mm2/s or higher at 40° C.
Type:
Application
Filed:
February 12, 2012
Publication date:
August 16, 2012
Applicants:
AOKI SCIENCE INSTITUTE CO., LTD, AISAN INDUSTRY CO., LTD., KOTOBUKI KINZOKU KOGYO CO., LTD., RYOBI LTD.
Abstract: The invention provides an oil type release agent die casting containing 70 to 98 parts by weight of a solvent having a specified flash point, 1 to 10 parts by weight of mineral oils and/or synthetic oils having a high viscosity, 15 parts by weight or less of a silicone oil, and 1 to 5 parts by weight of additives having a lubricating function, wherein the flash point of the agent is in the range of 70 to 170° C., and dynamic viscosity of the agent is 2 to 30 mm2/s or higher at 40° C., and a method for setting a mixing ratio of the solvent, a casting method, and a spraying unit for the case of using the release agent.
Type:
Grant
Filed:
February 8, 2007
Date of Patent:
February 14, 2012
Assignees:
Aoki Science Institute Co., Ltd., Ryobi Ltd., Kotobuki Kinzoku Kogyo Co., Ltd., Aisan Industry Co., Ltd.