Abstract: Patterned dies made of non-conductive resins may be equipped with integrated electrodes in different manners. It is proved to be difficult to produce high-quality electrodes especially in microstructured dies. A patterned plastic die arranged on a carrier plate is filled with a solution of a metal compound. This solution is irradiated through the carrier plate from the back side of the carrier plate using laser light, ultraviolet light or X-rays. The metal compound is transformed in the immediate vicinity of the base of the structure and a metal layer is deposited on the base of the structure forming the electrodes. The method is suitable for a base of the structure forming a coherent or a non-coherent area. Plastic dies containing integrated electrodes are used for electroless or electrophoretic deposition of materials and for electroplating, in all cases starting from the integrated electrodes, and for analytical methods.
Type:
Grant
Filed:
June 17, 1999
Date of Patent:
July 31, 2001
Assignee:
MicroParts Gesellschaft für Mikrostrukturtechnik
mbH
Abstract: The present invention concerns stepped mould inserts, a method of producing the same and high-precision stepped microstructure bodies moulded therewith. The present stepped mould inserts and method of producing the same are more simple than previous methods. The lithographically produced regions of a patterned resist layer, which are exposed by development on a flat plate, are filled with metal. The layer may be mechanically removed, down to a predetermined thickness. After the residues of the resist have been dissolved out, if necessary or desired, this operation is repeated from one to several times. The regions removed from the resist layer are filled with metal, covered and separated from the resist layer, thus providing a multistep metallic mould insert. High-precision microstructure bodies having a multistep structure are produced with the present stepped mould insert.
Type:
Grant
Filed:
April 2, 1996
Date of Patent:
February 10, 1998
Assignee:
MicroParts Gesellschaft fur Mikrostrukturtechnik mbH
Abstract: The present invention concerns stepped mould inserts, a method of producing the same and high-precision stepped microstructure bodies moulded therewith. The present stepped mould inserts and method of producing the same are more simple than previous methods. The lithographically produced regions of a patterned resist layer, which are exposed by development on a flat plate, are filled with metal. The layer may be mechanically removed, down to a predetermined thickness. After the residues of the resist have been dissolved out, if necessary or desired, this operation is repeated from one to several times. The regions removed from the resist layer are filled with metal, covered and separated from the resist layer, thus providing a multistep metallic mould insert. High-precision microstructure bodies having a multistep structure are produced with the present stepped mould insert.
Type:
Grant
Filed:
June 6, 1995
Date of Patent:
June 25, 1996
Assignee:
MicroParts Gesellschaft fur Mikrostrukturtechnik mbH
Abstract: A method of manufacturing passive integrated optical devices from polymeric materials, the method comprising providing a step structure at each transition between a fiber alignment structure and the preform for the light waveguide structure, wherein both of these structures are produced simultaneously. Passive integrated optical devices having ridges or trenches with rectangular cross sections and manufactured to this method are also described.
Type:
Grant
Filed:
March 8, 1993
Date of Patent:
May 10, 1994
Assignee:
Microparts Gesellschaft fur Mikrostrukturtechnik mbH