Abstract: An atmospheric leach process in the recovery of nickel and cobalt from lateritic ores, said processing including the steps of: a) separating the lateritic ore into a low magnesium containing ore fraction, and a high magnesium containing ore fraction by selective mining or post mining classification; b) separately slurrying the separated ore fractions; c) leaching the low magnesium containing ore fraction with concentrated sulphuric acid as a primary leach step; and d) introducing the high magnesium content ore slurry following substantial completion of the primary leach step and precipitating iron as goethite or another low sulphate containing form of iron oxide or iron hydroxide, wherein sulphuric acid released during iron precipitation is used to leach the high magnesium ore fraction as a secondary leach step.
Type:
Grant
Filed:
March 14, 2003
Date of Patent:
August 26, 2008
Assignee:
QNI Technology Pty. Ltd.
Inventors:
Houyuan Liu, James D. Gillaspie, Coralie Adele Lewis, David Neudorf, Steven Barnett
Abstract: A process is provided for the recovery of a metallic nickel product in a solvent extraction process which includes the steps of forming a nickel ammine complex by stripping nickel from a nickel loaded organic phase with a high strength ammonia solution and then reducing the nickel ammine complex with hydrogen from the high strength ammonia solution to produce a metallic nickel product. By virtue of the present process, a reductive precipitation of nickel by hydrogen is obtained so as to recover a metallic nickel product, and the process is advantageous in that it will allow for commercial processes wherein nickel may be recovered by hydrogen reduction based on high strength ammonia solutions.
Abstract: A process for producing a cobalt III encapsulated nickel hydroxide or basic nickel carbonate product including the steps of: (i) providing an ammoniacal solution including cobalt ammine complexes and nickel II ammine complexes; (ii) progressively lowering the ammonia content to sequentially precipate the nickel as an hydroxide or basic carbonate; and (iii) further lowering the ammonia content to precipitate the majority of the cobalt as cobalt III oxide hydroxide; wherein the majority of cobalt III oxide hydroxide coats on the surface of the precipitate nickel hydroxide or basic nickel carbonate to form a coated particle.
Type:
Grant
Filed:
August 7, 2003
Date of Patent:
September 11, 2007
Assignee:
QNI Technology Pty. Ltd.
Inventors:
John Ernest Fittock, Cheryl Christine Lucas, Katherine Fiona Howison
Abstract: A method of measuring the instantaneous parameters of a consumable electrode by: (a) providing a laser measuring device and positioning the laser measuring device in the vicinity of the electrode to be measured; (b) activating the laser measuring device to obtain data relating to the instantaneous parameters of the consumable electrode; and (c) transferring the data obtained from the laser measuring device to a computer data processing and storage device to determine the instantaneous parameters of the electrode.