Abstract: A thermal treatment process for an article of a cast or wrought aluminum-silicon alloy with an eutectic phase. The process comprises a rapid heating of the article to an annealing temperature of 400° C. to 555° C. and maintaining the article at this temperature for a not more than 14.8 minutes.
Abstract: A thermal treatment process for an article of a cast or wrought aluminum-silicon alloy with an eutectic phase. The process comprises a rapid heating of the article to an annealing temperature of 400° C. to 555° C. and maintaining the article at this temperature for a not more than 14.8 minutes.