Patents Assigned to San Fang Chemical Industry Co., Ltd.
-
Publication number: 20080200102Abstract: The present invention mainly relates to a polishing pad comprising a base material comprising fibers; a membrane with low permeability; and a buffer layer formed between the base material and an upper surface of the membrane with low permeability and embedded into the fibers of the base material. A method of polishing a substrate comprising using the polishing pad and a method for manufacturing the polishing pad as described above are also provided.Type: ApplicationFiled: February 15, 2007Publication date: August 21, 2008Applicant: San Fang Chemical Industry Co., Ltd.Inventors: Chung-Chih Feng, I-Peng Yao, Lyang-Gung Wang, Yung-Chang Hung
-
Publication number: 20080188168Abstract: The present invention relates to a polishing material having polishing particles and a method for making the same. The polishing material having polishing particles includes a base material, a plurality of polishing particles and a high polymer elastic body. The base material has a plurality of fibers for defining a plurality of grid-spaces. The polishing particles are distributed in the grid-spaces. The high polymer elastic body covers the base material and the polishing particles. Whereby, the polishing particles are uniformly distributed on a surface of a polishing workpiece during the polishing process. Furthermore, the base material prevents the polishing particles from contacting the polishing workpiece so as to avoid the scratch of the polishing workpiece. Also, the base material provides effects for sweeping the small grinded pieces.Type: ApplicationFiled: February 5, 2007Publication date: August 7, 2008Applicant: San Fang Chemical Industry Co., Ltd.Inventors: Chung-Chih Feng, I-Peng Yao, Lyang-Gung Wang, Yung-Chang Hung, Chao-Yuan Tsai
-
Publication number: 20080171493Abstract: The present invention mainly relates to a polishing pad and method of producing the same. The polishing pad comprises a base material having a surface for polishing a substrate, wherein the surface comprises a non-woven fabric and an elastomer. The non-woven fabric is made of a long fiber and the elastomer is embedded into the fabric.Type: ApplicationFiled: January 12, 2007Publication date: July 17, 2008Applicant: San Fang Chemical Industry Co., Ltd.Inventors: Chung-Chih Feng, I-Peng Yao, Chen-Hsiang Chao, Yung-Chang Hung
-
Patent number: 7361418Abstract: The present invention relates to a luminary material comprising a substrate; a luminary layer formed on a surface of the substrate; and a surface layer comprising a first portion and a second portion, wherein the first portion allows stronger light to be emitted from the luminary layer than the second portion. The luminary material according to the invention exhibits various colors, patterns and/or textures formed on the surface. Therefore, the luminary material is qualified as a decorative material in the light. A method for manufacturing the luminary material is also provided.Type: GrantFiled: June 1, 2006Date of Patent: April 22, 2008Assignee: San Fang Chemical Industry Co., Ltd.Inventors: Chung Chih Feng, Yuan Fang Tsai, Cheng Ming Lin, Chien Chia Huang
-
Publication number: 20080075938Abstract: A macromolecular laminate includes a main layer made of a first type of polyurethane resin compound that is liquid at room temperature. The first type of polyurethane resin compound is made through mixing polyurethane resin with solid content higher than 50% by weight with additives. An auxiliary layer may be formed on the main layer and made of a second type of polyurethane resin compound different from the first type of polyurethane resin compound.Type: ApplicationFiled: October 25, 2007Publication date: March 27, 2008Applicant: San Fang Chemical Industry Co., Ltd.Inventors: Ching-Tang Wang, Wu-Tsang Tsai, Lung-Chuan Wang, Chung-Chih Feng, Chun-Wei Wu
-
Patent number: 7316605Abstract: The present invention relates to a sheet for mounting a polishing workpiece. The sheet comprises a substrate and a surface layer. The substrate has a surface. The surface layer is located on the surface of the substrate, with no hole structure existing in the interior thereof, and has a plurality of through holes. Accordingly, when the polishing workpiece contacts the surface layer, the air therebetween is vented to the substrate via the through holes and then is easily vented out, without the phenomenon of air wrapping, which increases the adsorption force between the polishing workpiece and the sheet, thereby improving the polishing effect of the polishing workpiece.Type: GrantFiled: July 3, 2006Date of Patent: January 8, 2008Assignee: San Fang Chemical Industry Co., Ltd.Inventors: Chung-Chih Feng, I-Peng Yao, Chen-Hsiang Chao
-
Publication number: 20070218791Abstract: There is disclosed artificial leather with even imprinted texture and a method for making the same. The method includes the steps of: making a thermally imprintable polyurethane resin foil into a first substrate; providing at least one polyurethane resin layer on the first substrate in a spotted manner or by rolling or spraying; making pre-determined texture or graphics on the polyurethane resin layer by imprinting; making non-woven fabric, elastic fabric, woven fabric or ultra-fine fiber materials into a second substrate; and providing the first substrate on the second substrate by adhesion so as to form the artificial leather with even imprinted texture.Type: ApplicationFiled: July 27, 2006Publication date: September 20, 2007Applicant: SAN FANG CHEMICAL INDUSTRY CO., LTD.Inventors: Mao-Kan Lee, Zhing-Hung Chen, Ming-Chang Cheng, Yung-Hsiang Chou
-
Publication number: 20070207687Abstract: Artificial leather includes a substrate and a coating of a first elastomeric resin provided on the substrate. The substrate contains a second elastomeric resin evenly spread in the substrate. The first elastomeric resin forming the coating is identical to the second elastomeric resin in the substrate. The substrate includes a first porous structure. The coating includes a second porous structure contiguous to the first porous structure of the substrate. Preferably, the substrate has a density larger than that of the coating.Type: ApplicationFiled: February 28, 2007Publication date: September 6, 2007Applicant: San Fang Chemical Industry Co., LTD.Inventors: Ching-Tang Wang, Mong-Ching Lin, Chung-Chih Feng, Jung-Ching Chang, Hsien-Chang Hung, Ping-Liang Chiu, Chien-Te Wu
-
Publication number: 20070155268Abstract: A polishing pad includes a non-woven cloth and a continuous porous polymer. The non-woven cloth includes fibers. The polymer includes a plurality of holes communicated with one another. The polymer is cured in and bonded to the non-woven cloth. A surface of the polishing pad is constituted by the fibers of the non-woven cloth and the polymer.Type: ApplicationFiled: December 30, 2005Publication date: July 5, 2007Applicant: SAN FANG CHEMICAL INDUSTRY CO., LTD.Inventors: Chung-Ching Feng, Chen-Hsiang Chao, I-Peng Yao, Yung-Chang Hung, Jyh-Jen Lee
-
Publication number: 20060272770Abstract: Disclosed is a method for making artificial leather with superficial texture. In the method, a substrate is coated, in a non-overall manner, with a wet polyurethane resin. After curing, there is provided a polyurethane resin coated on releasing paper. Thus, a semi-product is made. Texture of the releasing paper is transferred to a surface of the semi-product. Then, the semi-product with the texture on the surface is coated with a layer of a chemical. A machine is used to heat and flatten the surface of the semi-product. Finally, the semi-product is physically finished by forces so that the surface of the final product is formed with texture like that of real leather.Type: ApplicationFiled: August 16, 2006Publication date: December 7, 2006Applicant: SAN FANG CHEMICAL INDUSTRY CO., LTD.Inventors: Mao-Kan Lee, Ming-Cheng Chang, Zhing-Hung Chen, Yung-Hsiang Chou
-
Publication number: 20060270329Abstract: A method is provided for making a polishing pad. In the method, ultrafine fiber-generating fibers are made into a non-woven fabric with two sides. At least one of the sides of the non-woven fabric is made a dense layer. The non-woven fabric is coated with a polymer. Because of the dense layer, the polymer cannot penetrate the non-woven fabric. The ultrafine fiber-generating fibers are converted to ultrafine fibers. Since the dense layer prevents the polymer from penetrating the ultrafine fiber-generating fibers, the ultrafine fibers remain a high concentration of fiber. The ultrafine fibers are transformed into nap. Therefore, the polishing pad is made with a polishing layer that includes the nap. The concentration of fiber of the polishing layer is higher than 80%.Type: ApplicationFiled: March 6, 2006Publication date: November 30, 2006Applicant: SAN FANG CHEMICAL INDUSTRY CO., LTD.Inventors: Chung-Chih Feng, Chen-Hsiang Chao, I-Peng Yao
-
Publication number: 20060263601Abstract: There is provided a method for splitting a split type conjugate fiber. The method includes four steps. Firstly, there is provided a first polymer with crystallization of 40% to 95% and a second polymer with crystallization of 1% to 25%. Secondly, a conjugate fiber is made of the first and second polymers by conjugate spinning. Thirdly, the conjugate fiber is submerged in water so that the conjugate fiber contains water. Finally, the conjugate fiber is heated and split into fine fibers.Type: ApplicationFiled: May 11, 2006Publication date: November 23, 2006Applicant: SAN FANG CHEMICAL INDUSTRY CO., LTD.Inventors: Lung-Chuan Wang, Chung-Chih Feng, Kuo-Kuang Cheng, Ta-Min Cheng, Chih-Yi Lin, Kuan-Hsiang Chang, Gao-Long Yang
-
Publication number: 20060249244Abstract: A method for producing an environmental friendly artificial leather product includes coating a first solvent-free elastomer resin composition on a releasing paper to form a top layer, coating a polyurethane resin composition containing more than 50% by weight solid content on the top layer to form an intermediate layer, coating a second solvent-free elastomer resin composition on the intermediate layer to form an adhesive layer, and finally applying a substrate on the adhesive layer, and peeling the releasing paper.Type: ApplicationFiled: July 14, 2006Publication date: November 9, 2006Applicant: San Fang Chemical Industry Co. LTD.Inventors: Ching-Tang Wang, Mong-Ching Lin, Chung-Chih Feng, Pei-Huo Huang, Yong-Song Lin
-
Publication number: 20060218729Abstract: There is disclosed a method for making environment-friendly artificial leather from ultra micro fiber without solvent treatment. The method includes the step of making at least two components into ultra micro fibers, as raw materials, by means of conjugate spinning. By means of spun lacing or water lacing, three-dimensional interlacing is conducted on the ultra micro fibers in order to provide non-woven fabric, as a substrate. After the substrate is impregnated with water-borne resin solution, salt solution is used to solidify the water-borne resin solution in the substrate. The sea component of the ultra micro fibers is removed by means of alkaline. Abrading and finishing are conducted in order to obtain a semi-product of the environment-friendly artificial leather.Type: ApplicationFiled: September 29, 2005Publication date: October 5, 2006Applicant: SAN FANG CHEMICAL INDUSTRY CO., LTD.Inventors: Chung-Chih Feng, Kuo-Kuang Cheng, Jong-Shy Lin, Chun-Hsien Lee
-
Publication number: 20060160449Abstract: There is disclosed a moisture-absorbing, quick drying, thermally insulating, elastic, composite material and a method for making the same. Adhesive is provided on the top and bottom of a highly porous foil so that the adhesive does not form a continuous film. By means of the adhesive, two sheets of elastic fabric are adhered to the top and bottom of the highly porous foil in order to provide a composite material. The composite material is low in density and high in porosity. As the adhesive does not form a continuous film, the composite material is highly porous and is called a moisture-absorbing, quick drying, thermally insulating, elastic, composite material.Type: ApplicationFiled: November 9, 2005Publication date: July 20, 2006Applicant: SAN FANG CHEMICAL INDUSTRY CO., LTD.Inventors: Ko-Feng Wang, I-Peng Yao, Kun-Lin Chiang
-
Publication number: 20060147642Abstract: A method for producing artificial leather includes providing a substrate with an upper surface and a lower surface, providing a coating of an elastomeric resin on the upper surface of the substrate, and providing a pressure difference between the upper and lower surfaces of the substrate so as to cause infiltration of the elastomeric resin into the substrate from the upper surface to the lower surface.Type: ApplicationFiled: March 15, 2006Publication date: July 6, 2006Applicant: San Fang Chemical Industry Co. LTD.Inventors: Ching-Tang Wang, Mong-Ching Lin, Chung-Chih Feng, Jung-Ching Chang, Hsien-Chang Hung, Ping-Liang Chiu, Chien-Te Wu
-
Patent number: 7025915Abstract: A method for producing an artificial leather includes mixed spinning an island polymer and a sea polymer having a different dissolving property from that of the island polymer at a predetermined temperature, producing a non-woven substrate from the fiber obtained, immersing the non-woven substrate into a polymer, dissolving and removing the sea polymer in the non-woven substrate to obtain an artificial leather as a semi-finished product, and polishing the surface of the artificial leather to obtain an artificial leather having excellent dyeability and advanced fluff-like property. The ratio of melt flow index of the sea polymer to relative viscosity of the island polymer is about 20 to about 55, in which the relative viscosity of the island polymer is about 2.7 to about 3.5 and the weight percentage of the sea polymer relative to the sum of the sea polymer and the island polymer is about 30% to about 70%.Type: GrantFiled: March 21, 2003Date of Patent: April 11, 2006Assignee: San Fang Chemical Industry Co., Ltd.Inventors: Ching-Tang Wang, Mong-Ching Lin, Chung-Chin Feng, Kuo-Kuang Cheng, Chin-Yi Lin
-
Publication number: 20060057432Abstract: Elastic artificial leather is disclosed. There are provided two polymers that include different crystallization degrees but similar fluidities. Fibers are made of the polymers. Non-woven cloth is made of the fibers. The non-woven cloth is soaked in water at 50 to 90° C. Thus, the fibers curl so that the non-woven cloth is elastic. The non-woven cloth is soaked in PU resin, washed and dried. Alternatively, the non-woven cloth includes, in addition to the fibers (“first type of fibers”), additional fibers (“second type of fibers”) that can be dissolved in water, alkali or solvent. The non-woven cloth is soaked in PU resin, washed and dried. The second type of fibers is removed from the non-woven cloth and the PU resin in order to leave elongated spaces. Thus, the artificial leather is elastic.Type: ApplicationFiled: April 14, 2005Publication date: March 16, 2006Applicant: SAN FANG CHEMICAL INDUSTRY CO., LTD.Inventors: Chung-Chih Feng, Kuo-Kuang Cheng, Chih-Yi Lin, Chiao-Fa Yang
-
Publication number: 20060046597Abstract: A method is disclosed for making permeable artificial leather that is realistic and permeable regarding air and liquid. At first, a non-woven cloth provided. A semi-product of the artificial leather is provided by means of immersing the non-woven cloth in a solution of a polymer resin. A highly porous sheet is provided. Finally, the final product of the artificial leather is provided by means of adhering the highly porous sheet to the semi-product of the artificial leather so that gaps exist between the highly porous sheet and the semi-product of the artificial leather.Type: ApplicationFiled: August 8, 2005Publication date: March 2, 2006Applicant: SAN FANG CHEMICAL INDUSTRY CO., LTD.Inventors: Ko-Feng Wang, I-Peng Yao, Mao-Kan Lee, Chen-Hsiang Chao, Zhing-Hwng Chen, Ming-Cheng Chang, Yung-Chang Hung
-
Publication number: 20050260416Abstract: An environmental friendly artificial leather product includes a substrate, an adhesive layer, an intermediate layer and a top layer. The artificial leather resides in that the top layer and adhesive layer is formed of a solvent-free elastomer resin composition and the intermediate layer provided between the top layer and adhesive layer is formed of a polyurethane resin composition containing more than 50% by weight solid content of polyurethane resin. A method for producing an environmental friendly artificial leather product includes coating a first solvent-free elastomer resin composition on a releasing paper to form a top layer, coating a polyurethane resin composition containing more than 50% by weight solid content on the top layer to form an intermediate layer, coating a second solvent-free elastomer resin composition on the intermediate layer to form an adhesive layer, and finally applying a substrate on the adhesive layer, and peeling the releasing paper.Type: ApplicationFiled: August 10, 2005Publication date: November 24, 2005Applicant: SAN FANG CHEMICAL INDUSTRY CO., LTD.Inventors: Ching-Tang Wang, Mong-Ching Lin, Chung-Ching Feng, Pei-Huo Huang, Yong-Song Lin