  • Patent number: 5110629
    Abstract: A heat stable bond between uncured urethane formulations and a rubber or synthetic rubber substrate is obtained by a method comprising coating the rubber surface with first a polyamine solution, then a peroxide solution and then a polyisocyanate-terminated monomer or prepolymer before applying the uncured urethane. While previously used bonds employing cyanoacrylate ester adhesives lose bond strength at elevated temperatures, the bond achieved in the present invention is stable throughout the operating temperature of the urethane.
    Type: Grant
    Filed: October 5, 1990
    Date of Patent: May 5, 1992
    Assignee: Synair Corporation
    Inventors: Edward N. Gomberg, Ahmed A. Zurkiya
  • Patent number: 5099900
    Abstract: A self-healing tire system containing a tire casing, a tacky sealant material, an inner tube and anti-tack material is described. In one embodiment, either the surface of the inner tube or the inner surface of the tire casing is coated with the tacky sealant material. The surface of the sealant, the opposing surface or both are coated with the anti-tack material. The anti-tack material renders the sealant non-tacky for a sufficient time so that the inner tube can be inserted and inflated. However, the anti-tack material allows the sealant surface to become tacky again thereby adhering to the tube and providing for sealing of the tube when it is punctured. In another embodiment, a release agent is contained between the sealant and the tire casing which facilitates removal of the sealant and tube from the tire casing.
    Type: Grant
    Filed: October 24, 1989
    Date of Patent: March 31, 1992
    Inventor: Edward N. Gomberg
  • Patent number: 4957573
    Abstract: A self-healing tire containing an inner tube is obtained by a method comprising coating either the surface of the tube or the inner surface of a tire casing with a tacky, non-flowing sealant material. Prior to insertion of the inner tube, the surface of the sealant or the opposing surface of the tube or casing or both are coated with a anti-tack material, such as a plasticizer for the sealant. The anti-tack material renders the sealant non-tacky for a period of time long enough for insertion and inflation of the tube. However, the anti-tack material allows the sealant surface to become tacky again thereby adhering the tube to the casing and providing for sealing of the tube when it is punctured.
    Type: Grant
    Filed: July 31, 1989
    Date of Patent: September 18, 1990
    Inventor: Edward N. Gomberg
  • Patent number: 4418093
    Abstract: The present invention relates to a method and apparatus for producing a liner of elastomeric material insitu in a pneumatic tire casing.
    Type: Grant
    Filed: March 26, 1982
    Date of Patent: November 29, 1983
    Assignee: Synair Corporation
    Inventors: Edward N. Gomberg, James O. B. Wright
  • Patent number: 4240852
    Abstract: A method wherein uncured urethane formulations are bonded to a cured rubber or synthetic rubber substrate in such a manner so as to provide greater bonding strength than has been achieved previously in urethane formulation bonding to rubber or synthetic rubber.
    Type: Grant
    Filed: February 19, 1980
    Date of Patent: December 23, 1980
    Assignee: Synair Corporation
    Inventors: Edward N. Gomberg, Dana W. Somesla
  • Patent number: 4071386
    Abstract: A substantially conventional tubeless or tube-type tire casing is mounted on a wheel and contains a centrifugally distributed solid elastic fill material which is deflation proof. A heat curable elastomer is injected into the casing in liquid form, the casing is pneumatically pressurized to seat upon the wheel rims, and the assembly is rotated to centrifugally distribute and position the liquid elastomer until it has cured. Alternatively, a pressurizable tube of relatively small diameter extends about the wheel within the casing and between the beads and rims of the casing and wheel. The tube is belted to limit its radially outward expansion and is filled with air at a pressure sufficient to securely hold the casing beads on the wheel rims. The elastic fill material may have characteristics providing a ride equivalent to a relatively low air pressure and at the same time, the casing will be securely locked to the wheel by relatively high pressure in the belted tube.
    Type: Grant
    Filed: February 25, 1976
    Date of Patent: January 31, 1978
    Assignee: Synair
    Inventor: Edward N. Gomberg
  • Patent number: RE29890
    Abstract: A flat free pneumatic tire comprising a casing and a void free elastomeric filling material, which filling material is a polyurethane of (a) prepolymer of organic polyisocyanate and defined polyether or defined polyester and (b) a defined polyether or defined polyester, in the absence of foam producing material in the reaction zone. The elastomeric filling material itself. A two container article (system) adapted for producing said void free filling material where one container has said prepolymer reactant and the other container has the polyether or polyester reactant, as required.
    Type: Grant
    Filed: November 14, 1977
    Date of Patent: January 30, 1979
    Assignee: Synair Corporation