  • Patent number: 8063260
    Abstract: The present invention relates to a solid phosphoric acid catalyst and a process for conversion of hydrocarbons using a solid phosphoric acid catalyst. The solid phosphoric acid catalyst comprises silicon orthophosphate, and has a silicon orthophosphate to silicon pyrophosphate ratio of at least about 5:1. The total pore volume of the solid phosphoric acid catalyst is at least about 0.17 cm3 per gram of catalyst, of which at least about 0.15 cm3 per gram is contributed by pores with diameter of at least about 10,000 ?.
    Type: Grant
    Filed: July 7, 2009
    Date of Patent: November 22, 2011
    Assignee: Sud-Chemie Inc.
    Inventors: Ling Xu, Wayne Turbeville, Gregory A. Korynta, Jeffrey L. Braden
  • Publication number: 20100069692
    Abstract: The present invention relates to a solid phosphoric acid catalyst and a process for conversion of hydrocarbons using a solid phosphoric acid catalyst. The solid phosphoric acid catalyst comprises silicon orthophosphate, and has a silicon orthophosphate to silicon pyrophosphate ratio of at least about 5:1. The total pore volume of the solid phosphoric acid catalyst is at least about 0.17 cm3 per gram of catalyst, of which at least about 0.15 cm3 per gram is contributed by pores with diameter of at least about 10,000 ?.
    Type: Application
    Filed: July 7, 2009
    Publication date: March 18, 2010
    Inventors: Ling Xu, Wayne Turbeville, Gregory A. Korynta, Jeffrey L. Braden
  • Patent number: 7557060
    Abstract: The present invention relates to a solid phosphoric acid catalyst and a process for conversion of hydrocarbons using a solid phosphoric acid catalyst. The solid phosphoric acid catalyst comprises silicon orthophosphate, and has a silicon orthophosphate to silicon pyrophosphate ratio of at least about 5:1. The total pore volume of the solid phosphoric acid catalyst is at least about 0.17 cm3 per gram of catalyst, of which at least about 0.15 cm3 per gram is contributed by pores with diameter of at least about 10,000 ?.
    Type: Grant
    Filed: June 29, 2007
    Date of Patent: July 7, 2009
    Assignee: Sud-Chemie Inc.
    Inventors: Ling Xu, Wayne Turbeville, Gregory A. Korynta, Jeffrey L. Braden
  • Publication number: 20090005623
    Abstract: The present invention relates to a solid phosphoric acid catalyst and a process for conversion of hydrocarbons using a solid phosphoric acid catalyst. The solid phosphoric acid catalyst comprises silicon orthophosphate, and has a silicon orthophosphate to silicon pyrophosphate ratio of at least about 5:1. The total pore volume of the solid phosphoric acid catalyst is at least about 0.17 cm3 per gram of catalyst, of which at least about 0.15 cm3 per gram is contributed by pores with diameter of at least about 10,000 ?.
    Type: Application
    Filed: June 29, 2007
    Publication date: January 1, 2009