Patent number: 10823314Abstract: Provided herein is a polyurethane tube having a small bending repulsive stress and superior inner-pressure creep characteristics in a flexible polyurethane tube. The present polyurethane tube has a bending repulsive stress of 0.035 N/mm2 or less, wherein the polyurethane tube is formed so that the difference between the storage elastic modulus E?30 at 30° C. and the storage elastic modulus E?80 at 80° C. is 15% or less of E?30.Type: GrantFiled: November 29, 2016Date of Patent: November 3, 2020Assignee: Junkosha Inc.Inventors: Keiji Yoda, Hiroji Oda
-
Publication number: 20180356010Abstract: Provided herein is a polyurethane tube having a small bending repulsive stress and superior inner-pressure creep characteristics in a flexible polyurethane tube. The present polyurethane tube has a bending repulsive stress of 0.035 N/mm2 or less, wherein the polyurethane tube is formed so that the difference between the storage elastic modulus E?30 at 30° C. and the storage elastic modulus E?80 at 80° C. is 15% or less of E?30.Type: ApplicationFiled: November 29, 2016Publication date: December 13, 2018Inventors: Keiji Yoda, Hiroji Oda
-
Patent number: 10006570Abstract: A pipe joint includes a joint main body, a cap nut, a sleeve, an insertion groove between a pipe body mounting section and an external thread section of the joint main body, and an elastic member disposed in the insertion groove. When the external thread section and an internal thread section of the cap nut are screwed, the end face of the distal end side of the sleeve comes into contact with one end face of the elastic member to compress the elastic member, and the elastic member presses, with a self-repulsion force, the end face of the distal end side of the sleeve in the axial direction. Then, an inner circumferential surface of a proximal end side of the sleeve compresses the pipe body in a radial direction of the pipe body through a reaction force received from a fitting surface of the cap nut.Type: GrantFiled: June 20, 2014Date of Patent: June 26, 2018Assignee: JUNKOSHA INC.Inventors: Keiji Yoda, Hiroji Oda
-
Publication number: 20160131286Abstract: A pipe joint includes a joint main body, a cap nut, a sleeve, an insertion groove between a pipe body mounting section and an external thread section of the joint main body, and an elastic member disposed in the insertion groove. When the external thread section and an internal thread section of the cap nut are screwed, the end face of the distal end side of the sleeve comes into contact with one end face of the elastic member to compress the elastic member, and the elastic member presses, with a self-repulsion force, the end face of the distal end side of the sleeve in the axial direction. Then, an inner circumferential surface of a proximal end side of the sleeve compresses the pipe body in a radial direction of the pipe body through a reaction force received from a fitting surface of the cap nut.Type: ApplicationFiled: June 20, 2014Publication date: May 12, 2016Applicant: JUNKOSHA INC.Inventors: keiji YODA, Hiroji ODA
-
Patent number: 8222348Abstract: An epoxy silicon, which comprises at least a compound represented by the following general formula (1), and a compound represented by the following general formula (2); and which is represented by an average composition formula (3), wherein a value of [g/(a+b+c+d+e+f+g+h+i+j)] falls within a range of 0.020 or less.Type: GrantFiled: April 15, 2008Date of Patent: July 17, 2012Assignee: Asahi Kasei Chemicals CorporationInventors: Yoshito Kuroda, Masako Yokoyama, Hiroji Oda
-
Publication number: 20100120975Abstract: An epoxy silicon, which comprises at least a compound represented by the following general formula (1), and a compound represented by the following general formula (2); and which is represented by an average composition formula (3), wherein a value of [g/(a+b+c+d+e+f+g+h+i+j)] falls within a range of 0.020 or less.Type: ApplicationFiled: April 15, 2008Publication date: May 13, 2010Applicant: Asahi Kasei Chemicals CorporationInventors: Yoshito Kuroda, Masako Yokoyama, Hiroji Oda
-
Patent number: 7514520Abstract: A process for producing a phosphonitrilic acid ester. The process comprises using a specific compound as a catalyst to react phosphonitrile dichloride with at least one member selected among phenol compounds and/or alcohol compounds in the presence of a reaction solvent. Alternatively, the process comprises reacting a liquid reaction mixture obtained in a first stage with at least one member selected among phenol compounds and/or alcohol compounds without isolating phosphonitrile dichloride from the mixture.Type: GrantFiled: June 3, 2004Date of Patent: April 7, 2009Assignee: Asahi Kasei Chemicals CorporationInventors: Kotaro Kuwata, Hiroji Oda
-
Publication number: 20070060739Abstract: A process for producing a phosphonitrilic acid ester. The process comprises using a specific compound as a catalyst to react phosphonitrile dichloride with at least one member selected among phenol compounds and/or alcohol compounds in the presence of a reaction solvent. Alternatively, the process comprises reacting a liquid reaction mixture obtained in a first stage with at least one member selected among phenol compounds and/or alcohol compounds without isolating phosphonitrile dichloride from the mixture.Type: ApplicationFiled: June 3, 2004Publication date: March 15, 2007Inventors: Kotaro Kuwata, Hiroji Oda
-
Patent number: 6825264Abstract: Disclosed is a flame retardant resin composition comprising: 100 parts by weight of a resin component (A) which is a resin mixture of an aromatic polycarbonate and a styrene polymer, wherein the resin mixture has an aromatic polycarbonate content of from 50 to 95% by weight and a styrene polymer content of from 5 to 50% by weight; 0.1 to 30 parts by weight of an organopolysiloxane (B) which comprises 0 to 70 mol % of a monofunctional siloxane unit (M unit), 0 to 100 mol % of a bifunctional recurring siloxane unit (D unit), 0 to 100 mol % of a trifunctional recurring siloxane unit (T unit), and 0 to 63 mol % of a tetrafunctional recurring siloxane unit (Q unit); and 0.0005 to 5 parts by weight of at least one inorganic metal salt (C) selected from the group consisting of inorganic alkali metal salts and inorganic alkaline earth metal salts.Type: GrantFiled: October 11, 2002Date of Patent: November 30, 2004Assignees: Asahi Kasei Chemicals Corporation, Wacker-Chemie Gesellschaft mit Beschrankter HaftungInventors: Hiroji Oda, Kotaro Kuwata
-
Publication number: 20030109660Abstract: Disclosed is a flame retardant resin composition comprising: 100 parts by weight of a resin component (A) which is a resin mixture of an aromatic polycarbonate and a styrene polymer, wherein the resin mixture has an aromatic polycarbonate content of from 50 to 95% by weight and a styrene polymer content of from 5 to 50% by weight; 0.1 to 30 parts by weight of an organopolysiloxane (B) which comprises 0 to 70 mol % of a monofunctional siloxane unit (M unit), 0 to 100 mol % of a bifunctional recurring siloxane unit (D unit), 0 to 100 mol % of a trifunctional recurring siloxane unit (T unit), and 0 to 63 mol % of a tetrafunctional recurring siloxane unit (Q unit); and 0.0005 to 5 parts by weight of at least one inorganic metal salt (C) selected from the group consisting of inorganic alkali metal salts and inorganic alkaline earth metal salts.Type: ApplicationFiled: October 11, 2002Publication date: June 12, 2003Inventors: Hiroji Oda, Kotaro Kuwata
-
Patent number: 6541548Abstract: There is provided an aromatic polycarbonate resin composition which exhibits high flame retardancy without sacrificing melt-molding stability or melt fluidity when molding the resin composition. The flame retardant aromatic polycarbonate resin composition comprises a resin component (a) comprising an aromatic polycarbonate and optionally a styrene polymer, the resin composition having an aromatic polycarbonate content of 20% by weight or more; and 0.1 to 50 parts by weight of an organopolysiloxane (b) comprising a linear organopolysiloxane (b)i and a cyclic organopolysiloxane (b)ii, component (b)ii present in an amount of from 5 to 95% by weight based on the total weight of components (b)i and (b)ii.Type: GrantFiled: August 2, 2001Date of Patent: April 1, 2003Assignees: Wacker-Chemie GmbH, Asahi Kasei Kabushiki KaishaInventors: Richard Weidner, Hiroji Oda
-
Publication number: 20020037966Abstract: There is provided an aromatic polycarbonate resin composition which exhibits high flame retardancy without sacrificing melt-molding stability or melt fluidity when molding the resin composition. The flame retardant aromatic polycarbonate resin composition comprises a resin component (a) comprising an aromatic polycarbonate and optionally a styrene polymer, the resin composition having an aromatic polycarbonate content of 20% by weight or more; and 0.1 to 50 parts by weight of an organopolysiloxane (b) comprising a linear organopolysiloxane (b)i and a cyclic organopolysiloxane (b)ii, component (b)ii present in an amount of from 5 to 95% by weight based on the total weight of components (b)i and (b)ii.Type: ApplicationFiled: August 2, 2001Publication date: March 28, 2002Inventors: Richard Weidner, Hiroji Oda
-
Patent number: 5352745Abstract: A novel curable polyphenylene ether resin composition caontains (a) a curable polyphenylene ether resin containing at least a reaction product of a polyphenylene ether with an unsaturated carboxylic acid or an acid anhydride, (b) at least one cyanurate selected from the group consisting of triallyl isocyanurate and triallyl cyanurate, optionally (c) a resin composition comprising an epoxy resin and a curing agent and/or (d) a compound having at least one unsaturated double bond and at least one epoxy group and/or (e) a reinforcement material. The resin composition has excellent film-forming properties, resin flowability in pressing and storage stability. A cured polyphenylene ether resin composition obtained by curing the curable polyphenylene ether resin composition has excellent chemical resistance, heat resistance, dielectric properties and dimensional stability.Type: GrantFiled: November 3, 1993Date of Patent: October 4, 1994Assignee: Asahi Kasei Kogyo Kabushiki KaishaInventors: Teruo Katayose, Yoshiyuki Ishii, Hiroji Oda
-
Patent number: 5218030Abstract: A novel curable polyphenylene ether resin composition is disclosed, which comprises (a) a curable polyphenylene ether resin having at least one group selected from the group consisting of an allyl group and a propargyl group and (b) at least one cyanurate. The resin composition has excellent storage stability, film-forming properties and melt moldability. If desired, a fire retardant, optionally together with an antimony-containing auxiliary fire retardant, and/or a reinforcement is incorporated into the resin composition in order to improve the fire retardance and mechanical properties of the resin composition, respectively. By curing the resin composition, a cured polyphenylene ether resin composition comprising a chloroform nonextractable polyphenylene ether resin component and a chloroform extractable, polyphenylene ether-containing component is obtained, which has excellent chemical resistance, electrical properties, dimensional stability and heat resistance.Type: GrantFiled: February 7, 1990Date of Patent: June 8, 1993Assignee: Asahi Kasei Kogyo Kabushiki KaishaInventors: Teruo Katayose, Hiroji Oda, Haruhisa Sasaki
-
Polyphenylene ether resin comprising chloroform extractable/nonextractable polyphenylene ether resin
Patent number: 4923932Abstract: A novel cured polyphenylene ether resin is disclosed comprising a chloroform nonextractable polyphenylene ether and a chloroform extractable polyphenylene ether. By subjecting the resin to pyrolysis gas chromatography, the resin is decomposed to form 3,5-dimethylphenol specifically. The chloroform extractable polyphenylene ether is contained in the resin in an amount of 0.01 to 20% by weight and comprises polyphenylene ether units substituted by an alkenyl group and/or an alkynyl group. The novel cured polyphenylene ether resin has excellent mechanical properties, electrical properties, heat resistance and chemical resistance. The cured polyphexylene ether resin is prepared by curing a novel curable polyphenylene ether resin comprising polyphenylene ether units substituted with an alkenyl groups and/or an alkynyl groups at a specific average substitution degree.Type: GrantFiled: September 9, 1988Date of Patent: May 8, 1990Assignee: Asahi Kasei Kogyo Kabushiki KaishaInventors: Teruo Katayose, Hiroji Oda -
Patent number: 4820787Abstract: A shaped article composed of an at least biaxially orientated tetrafluoroethylene polymer of ultrahigh molecular weight, which has a draw ratio of at least 3.0, a specific gravity of at least 1.8 and an orientation release stress at 200.degree. C. of at least 5 Kg/cm.sup.2. The shaped article has excellent creep resistant and gas barrier properties, and can advantageously be utilized as a sealant, a lining material, a bearing pad, a sliding pad or the like. The shaped article may be produced by compressing a preformed sheet of a tetrafluoroethylene polymer at a temperature of from 170.degree. to 400.degree. C., under such conditions that plug flow of the polymer is produced, followed by cooling in the compressed state.Type: GrantFiled: March 18, 1987Date of Patent: April 11, 1989Assignee: Asahi Kasei Kogyo Kabushiki KaishaInventors: Hiroshi Kataoka, Kinya Matsuzawa, Hiroji Oda