Abstract: The present invention relates to the dielectric composition including barium titanate, strontium titanate, titanium oxide and bismuth oxide. In case when the content of barium titanate, converted to BaTiO3, is a mol %, the content of strontium titanate, converted to SrTiO3, is b mol %, the content of titanium oxide and bismuth oxide, converted to Bi2Ti3O9, is c mol %, and a+b+c=100, a, b and c are values within a scope surrounded by the following four points, i.e. point A, point B, point C and point D in a three-dimensional phase diagram. Point A: (a, b, c)=(52.1, 40.0, 7.9); point B: (a, b, c)=(86.5, 5.6, 7.9); point C: (a, b, c)=(91.0, 5.6, 3.4); point D: (a, b, c)=(56.6, 40.0, 3.4).
Type:
Grant
Filed:
December 28, 2017
Date of Patent:
July 9, 2019
Assignees:
TDK CORPORATION, TDK XIAMEN CO., LTD.
Inventors:
Guibin Ge, RuiLun Zhang, Fan Zhang, Jintao Huang, Kazuya Muto, Daisuke Ohtsu, Kakeru Watanabe
Publication number: 20180179078
Abstract: The present invention relates to the dielectric composition including barium titanate, strontium titanate, titanium oxide and bismuth oxide. In case when the content of barium titanate, converted to BaTiO3, is a mol %, the content of strontium titanate, converted to SrTiO3, is b mol %, the content of titanium oxide and bismuth oxide, converted to Bi2Ti3O9, is c mol %, and a+b+c=100, a, b and c are values within a scope surrounded by the following four points, i.e. point A, point B, point C and point D in a three-dimensional phase diagram. Point A: (a, b, c)=(52.1, 40.0, 7.9); point B: (a, b, c)=(86.5, 5.6, 7.9); point C: (a, b, c)=(91.0, 5.6, 3.4); point D: (a, b, c)=(56.6, 40.0, 3.4).
Type:
Application
Filed:
December 28, 2017
Publication date:
June 28, 2018
Applicants:
TDK CORPORATION, TDK XIAMEN CO., LTD.
Inventors:
Guibin GE, RuiLun ZHANG, Fan ZHANG, Jintao HUANG, Kazuya MUTO, Daisuke OHTSU, Kakeru WATANABE