Patents by Inventor Kelly Ahlgren

Kelly Ahlgren has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 11453765
    Abstract: A heat-shrinkable film comprises a blend of 35-75 wt % of an ethylene-based polymer, 10-45 wt % of an ethylene/unsaturated ester copolymer, and 5-30 wt % of a plastomer, with the blend making up at least 20 wt % of the film. The ethylene-based polymer has a peak melt point ?95° C. The plastomer has a peak melt point ?90° C. and a melt index of ?1.1 g/10 min. The film comprises a cross-linked polymer network which has been strained by solid state orientation. The film has a total free shrink at 85° C. of at least 90% and an energy-to-break of at least 0.70 J/mil.
    Type: Grant
    Filed: April 13, 2018
    Date of Patent: September 27, 2022
    Assignee: Cryovac, LLC
    Inventors: Ashley Wynne, Kelly Ahlgren, Miles Johnston, Rebecca Higginbotham
  • Patent number: 11305520
    Abstract: A multilayer, heat-shrinkable film has a first portion containing an outer heat seal layer and a second portion containing a PVDC barrier layer and a second outer layer comprising polyester. Both film portions comprise polymer networks which are strained by solid-state orientation, but only the first portion contains a crosslinked polymer network. The film has (i) a total free shrink at 85° C. of at least 90% and (ii) an instrumented impact energy-to-break of at least 0.0.65 J/mil and/or an instrumented impact peak load of at least 70 N/mil. The film is primarily made from ethylene-based polymers. Packaging articles can be made by sealing the film to itself. The film comprises no polyamide or polyamide in an amount up to 10 wt %, on a total film weight basis.
    Type: Grant
    Filed: April 13, 2018
    Date of Patent: April 19, 2022
    Assignee: Cryovac, LLC
    Inventors: Ashley Wynne, Kelly Ahlgren, Miles Johnston, Rebecca Kersey
  • Publication number: 20210114356
    Abstract: A packaging article comprises a heat-shrinkable film having a total free shrink at 85° C. of at least 90%. The film has an inside seal layer, an outside polyester layer, and an inner oxygen barrier layer. A portion of the film contains a crosslinked polymer network. At least one film layer comprises an incompatible polymer blend. The article has tear initiators. The package provides post-shrink, full-length tear from the tear initiators to the opposite edge of the article, for easy product removal. The film has an instrumented impact energy-to-break of at least 0.65 J/mil, and/or an instrumented impact peak load strength of at least 66 Newtons/mil, and/or Truburst strength of at least 8 psi/mil.
    Type: Application
    Filed: April 12, 2018
    Publication date: April 22, 2021
    Inventors: Ashley Wynne, Kelly Ahlgren, Miles Johnston, Rebecca Kersey
  • Publication number: 20210101374
    Abstract: A multilayer, heat-shrinkable film has a first portion containing an outer heat seal layer and a second portion containing a PVDC barrier layer and a second outer layer comprising polyester. Both film portions comprise polymer networks which are strained by solid-state orientation, but only the first portion contains a crosslinked polymer network. The film has (i) a total free shrink at 85° C. of at least 90% and (ii) an instrumented impact energy-to-break of at least 0.0.65 J/mil and/or an instrumented impact peak load of at least 70 N/mil. The film is primarily made from ethylene-based polymers. Packaging articles can be made by sealing the film to itself. The film comprises no polyamide or polyamide in an amount up to 10 wt %, on a total film weight basis.
    Type: Application
    Filed: April 13, 2018
    Publication date: April 8, 2021
    Inventors: Ashley Wynne, Kelly Ahlgren, Miles Johnston, Rebecca Kersey
  • Publication number: 20200062938
    Abstract: A heat-shrinkable film comprises a blend of 35-75 wt % of an ethylene-based polymer, 10-45 wt % of an ethylene/unsaturated ester copolymer, and 5-30 wt % of a plastomer, with the blend making up at least 20 wt % of the film. The ethylene-based polymer has a peak melt point ?95° C. The plastomer has a peak melt point ?90° C. and a melt index of ?1.1 g/10 min. The film comprises a cross-linked polymer network which has been strained by solid state orientation. The film has a total free shrink at 85° C. of at least 90% and an energy-to-break of at least 0.70 J/mil.
    Type: Application
    Filed: April 13, 2018
    Publication date: February 27, 2020
    Inventors: Ashley Wynne, Kelly Ahlgren, Miles Johnston, Rebecca Kersey