Patents by Inventor Max A. Kaplan

Max A. Kaplan has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Publication number: 20240110270
    Abstract: A method for heat treating a superalloy component includes heating a superalloy component to a first temperature, cooling the superalloy from the first temperature to a second temperature at a first cooling rate in a furnace, and cooling the superalloy component from the second temperature to a final temperature at a second cooling rate. The second cooling rate is higher than the first cooling rate.
    Type: Application
    Filed: October 6, 2023
    Publication date: April 4, 2024
    Inventors: Max A. Kaplan, Mario P. Bochiechio, Stephen D. Rittenburg, Paul D. Bennett
  • Patent number: 11826849
    Abstract: A joining method includes performing a first heat treatment step on a first superalloy workpiece and a second superalloy workpiece wherein at least one of the first and second superalloy workpieces include a gamma matrix phase and a gamma-prime precipitate phase. The first and second superalloy workpieces are joined using a solid state joining process, subjected to a post-weld stress relief operation and a final aging heat treatment.
    Type: Grant
    Filed: February 11, 2021
    Date of Patent: November 28, 2023
    Assignee: RTX Corporation
    Inventors: Ashwin Raghavan, Enrique E. Montero, Max A. Kaplan, Eli N. Ross, Mario P. Bochiechio
  • Publication number: 20210316392
    Abstract: A joining method includes performing a first heat treatment step on a first superalloy workpiece and a second superalloy workpiece wherein at least one of the first and second superalloy workpieces include a gamma matrix phase and a gamma-prime precipitate phase. The first and second superalloy workpieces are joined using a solid state joining process, subjected to a post-weld stress relief operation and a final aging heat treatment.
    Type: Application
    Filed: February 11, 2021
    Publication date: October 14, 2021
    Inventors: Ashwin Raghavan, Enrique E. Montero, Max A. Kaplan, Eli N. Ross, Mario P. Bochiechio
  • Patent number: 10946476
    Abstract: A joining method includes performing a first heat treatment step on a first superalloy workpiece and a second superalloy workpiece wherein at least one of the first and second superalloy workpieces include a gamma matrix phase and a gamma-prime precipitate phase. The first and second superalloy workpieces are joined using a solid state joining process, subjected to a post-weld stress relief operation and a final aging heat treatment.
    Type: Grant
    Filed: May 11, 2017
    Date of Patent: March 16, 2021
    Assignee: Raytheon Technologies Corporation
    Inventors: Ashwin Raghavan, Enrique E. Montero, Max A. Kaplan, Eli N. Ross, Mario P. Bochiechio
  • Patent number: 10793934
    Abstract: An embodiment of a superalloy composition includes 1.5 to 4.5 wt % Al; 0.005 to 0.06 wt % B; 0.02 to 0.07 wt % C; 21.0 to 26.0 wt % Co; 11.5 to 16.0 wt % Cr; 8.50 to 19.0 wt % Ta; 0.005-0.10 wt % Zr; and balance Ni and incidental impurities.
    Type: Grant
    Filed: May 2, 2017
    Date of Patent: October 6, 2020
    Inventors: Max A. Kaplan, Xuan Liu, David Ulrich Furrer
  • Patent number: 10718041
    Abstract: A method for welding a first powder metallurgical (PM) part to a second powder metallurgical (PM) part includes: working a first face of the first PM part; working a first face of the second PM part; and friction welding the first face of the first part to the first face of the second part.
    Type: Grant
    Filed: June 26, 2017
    Date of Patent: July 21, 2020
    Assignee: Raytheon Technologies Corporation
    Inventors: Ashwin Sreekant Raghavan, Kenneth A. Frisk, Max A. Kaplan, Mario P. Bochiechio, Michael A. Czywczynski
  • Patent number: 10718042
    Abstract: A method for heat treating a superalloy component includes heating a superalloy component to a first temperature, cooling the superalloy from the first temperature to a second temperature at a first cooling rate in a furnace, and cooling the superalloy component from the second temperature to a final temperature at a second cooling rate. The second cooling rate is higher than the first cooling rate.
    Type: Grant
    Filed: June 28, 2017
    Date of Patent: July 21, 2020
    Assignee: United Technologies Corporation
    Inventors: Max A. Kaplan, Mario P. Bochiechio, Stephen D. Rittenburg, Paul D. Bennett
  • Publication number: 20200216939
    Abstract: A method for heat treating a superalloy component includes heating a superalloy component to a first temperature, cooling the superalloy from the first temperature to a second temperature at a first cooling rate in a furnace, and cooling the superalloy component from the second temperature to a final temperature at a second cooling rate. The second cooling rate is higher than the first cooling rate.
    Type: Application
    Filed: March 13, 2020
    Publication date: July 9, 2020
    Inventors: Max A. Kaplan, Mario P. Bochiechio, Stephen D. Rittenburg, Paul D. Bennett
  • Publication number: 20190063256
    Abstract: An embodiment of a superalloy composition includes 0 to 3.5 wt % Al; 0.005 to 0.05 wt % B; 0.005 to 0.25 wt % C; 10 to 27 wt % Co; 12 to 20 wt % Cr; 6 to 10 wt % Ti; 0.01 to 0.1 wt % Zr; and balance Ni and incidental impurities.
    Type: Application
    Filed: August 31, 2017
    Publication date: February 28, 2019
    Inventors: Max A. Kaplan, Xuan Liu, David Ulrich Furrer
  • Publication number: 20190003026
    Abstract: A method for heat treating a superalloy component includes heating a superalloy component to a first temperature, cooling the superalloy from the first temperature to a second temperature at a first cooling rate in a furnace, and cooling the superalloy component from the second temperature to a final temperature at a second cooling rate. The second cooling rate is higher than the first cooling rate.
    Type: Application
    Filed: June 28, 2017
    Publication date: January 3, 2019
    Inventors: Max A. Kaplan, Mario P. Bochiechio, Stephen D. Rittenburg, Paul D. Bennett
  • Publication number: 20180371594
    Abstract: A method for welding a first powder metallurgical (PM) part to a second powder metallurgical (PM) part includes: working a first face of the first PM part; working a first face of the second PM part; and friction welding the first face of the first part to the first face of the second part.
    Type: Application
    Filed: June 26, 2017
    Publication date: December 27, 2018
    Inventors: Ashwin Sreekant Raghavan, Kenneth A. Frisk, Max A. Kaplan, Mario P. Bochiechio, Michael A. Czywczynski
  • Publication number: 20180326533
    Abstract: A joining method includes performing a first heat treatment step on a first superalloy workpiece and a second superalloy workpiece wherein at least one of the first and second superalloy workpieces include a gamma matrix phase and a gamma-prime precipitate phase. The first and second superalloy workpieces are joined using a solid state joining process, subjected to a post-weld stress relief operation and a final aging heat treatment.
    Type: Application
    Filed: May 11, 2017
    Publication date: November 15, 2018
    Inventors: Ashwin Raghavan, Enrique E. Montero, Max A. Kaplan, Eli N. Ross, Mario P. Bochiechio
  • Publication number: 20180320254
    Abstract: An embodiment of a superalloy composition includes 1.5 to 4.5 wt % Al; 0.005 to 0.06 wt % B; 0.02 to 0.07 wt % C; 21.0 to 26.0 wt % Co; 11.5 to 16.0 wt % Cr; 8.50 to 19.0 wt % Ta; 0.005-0.10 wt % Zr; and balance Ni and incidental impurities.
    Type: Application
    Filed: May 2, 2017
    Publication date: November 8, 2018
    Inventors: Max A. Kaplan, Xuan Liu, David Ulrich Furrer