  • Patent number: 7874471
    Abstract: Provided are butt welds and methods of making such butt welds using a combination of fusion root welding and friction stir welding to yield welds with decreased propensity for dropout during friction stir welding without the need for a back-up support plate. In one form of the present disclosure, the butt weld includes: two or more abutting structural steel components beveled on faying surfaces on one side of the components to form a suitably shaped fusion root weld groove and unbeveled on faying surfaces on the opposite side of the components and interconnected with a first fusion root weld on the beveled side of the components and a second friction stir weld on the unbeveled side of the components, wherein the first fusion root weld has a width ranging from 7 mm to 30 mm, a penetration depth ranging from 2 mm to 20 mm, and an overfill ranging from 2 mm to 5 mm, and wherein the stir zone of the second friction stir weld penetrates the first fusion root weld.
    Type: Grant
    Filed: December 17, 2009
    Date of Patent: January 25, 2011
    Assignee: ExxonMobil Research and Engineering Company
    Inventors: Douglas Paul Fairchild, Steven Jeffrey Ford, Amit Kumar, Nathan Eugene Nissley, Nicholas E. Biery, Mario L. Macia
  • Publication number: 20100159265
    Abstract: Provided are butt welds and methods of making such butt welds using a combination of fusion root welding and friction stir welding to yield welds with decreased propensity for dropout during friction stir welding without the need for a back-up support plate. In one form of the present disclosure, the butt weld includes: two or more abutting structural steel components beveled on faying surfaces on one side of the components to form a suitably shaped fusion root weld groove and unbeveled on faying surfaces on the opposite side of the components and interconnected with a first fusion root weld on the beveled side of the components and a second friction stir weld on the unbeveled side of the components, wherein the first fusion root weld has a width ranging from 7 mm to 30 mm, a penetration depth ranging from 2 mm to 20 mm, and an overfill ranging from 2 mm to 5 mm, and wherein the stir zone of the second friction stir weld penetrates the first fusion root weld.
    Type: Application
    Filed: December 17, 2009
    Publication date: June 24, 2010
    Inventors: Douglas Paul Fairchild, Steven Jeffrey Ford, Amit Kumar, Nathan Eugene Nissley, Nicholas E. Biery, Mario L. Macia