    Abstract: A method for producing steel products (1) with optimum surface quality wherein the molten steel (1b) is produced in a process route (10, 100; 12; 13) that is selected according to a desired final microstructure (9), by melting in a furnace (2b) with an electrode system (31), and in a vacuum degassing system; or by melting in a furnace installation (35) or an individual furnace vessel (30), in a ladle furnace (25), and in a differential-pressure vacuum degassing system (43); or by melting in a furnace (2b) with additions of alloying materials (26), a partial-quantity degassing in the ladle furnace (25), or a vacuum degassing system (27) and a ladle degassing (27).
    Type: Grant
    Filed: February 13, 2009
    Date of Patent: September 20, 2011
    Assignee: SMS Siemag Aktiengesellschaft
    Inventors: Fritz-Peter Pleschiutschnigg, Karl-Ernst Hensger, Dieter Rosenthal, Rainer Teworte, Dieter Tembergen
  • Patent number: 7998237
    Abstract: Disclosed are a method and an installation for producing steel products (1) having an optimum surface quality, especially extremely low carbon contents (UCL steel or IF steel), nitrogen contents, total oxygen contents, high-strength or stainless steel qualities.
    Type: Grant
    Filed: May 25, 2004
    Date of Patent: August 16, 2011
    Assignee: SMS Siemag Aktiengesellschaft
    Inventors: Fritz-Peter Pleschiutschnigg, Karl-Ernst Hensger, Dieter Rosenthal, Rainer Teworte, Dieter Tembergen
  • Publication number: 20100000062
    Abstract: A method for producing steel products (1) with optimum surface quality wherein the molten steel (1b) is produced in a process route (10, 100; 12; 13) that is selected according to a desired final microstructure (9), by melting in a furnace (2b) with an electrode system (31), and in a vacuum degassing system; or by melting in a furnace installation (35) or an individual furnace vessel (30), in a ladle furnace (25), and in a differential-pressure vacuum degassing system (43); or by melting in a furnace (2b) with additions of alloying materials (26), a partial-quantity degassing in the ladle furnace (25), or a vacuum degassing system (27) and a ladle degassing (27).
    Type: Application
    Filed: February 13, 2009
    Publication date: January 7, 2010
    Inventors: Fritz-Peter Pleschiutschnigg, Karl-Ernst Hensger, Dieter Rosenthal, Rainer Teworte, Dieter Tembergen
  • Publication number: 20070272054
    Abstract: Disclosed are a method and an installation for producing steel products (1) having an optimum surface quality, especially extremely low carbon contents (UCL steel or IF steel), nitrogen contents, total oxygen contents, high-strength or stainless steel qualities.
    Type: Application
    Filed: May 25, 2004
    Publication date: November 29, 2007
    Inventors: Fritz-Peter Pleschiutschnigg, Karl-Ernst Hensger, Dieter Rosenthal, Rainer Teworte, Dieter Tembergen
  • Publication number: 20040154437
    Abstract: Molten steel is degasified under vacuum and in the first 5 minutes of the degasification to improve and accelerate the degasification solids in the form of pieces of a size of 2 to 50 mm are introduced into the melt.
    Type: Application
    Filed: December 4, 2003
    Publication date: August 12, 2004
    Applicant: SMS Mevac GmbH
    Inventors: Rainer Dittrich, Rainer Teworte, Dieter Tembergen