  • Patent number: 8920974
    Abstract: Disclosed is a cathode material comprising a mixture of an oxide powder (a) defined herein and an oxide powder (b) selected from the group consisting of an oxide powder (b1) defined herein and an oxide powder (b2) defined herein and a combination thereof wherein a mix ratio of the two oxide powders (oxide powder (a):oxide powder (b)) is 50:50 to 90:10. The cathode material uses a combination of an oxide powder (a) and 50% or less of an oxide powder (b) which can exert high capacity, high cycle stability, superior storage stability and high-temperature stability, thus advantageously exhibiting high energy density and realizing high capacity batteries.
    Type: Grant
    Filed: November 4, 2013
    Date of Patent: December 30, 2014
    Assignee: LG Chem, Ltd.
    Inventors: Suengeun Choi, Eunyoung Goh, Hyang Mok Lee, Heegyoung Kang, Sangbaek Ryu, Kiwoong Kim
  • Patent number: 8870978
    Abstract: Provided is a method for fabrication of a jelly-roll type electrode assembly having a cathode/separation membrane/anode laminate structure, including: (a) coating both sides of a porous substrate with organic/inorganic composite layers, each of which includes inorganic particles and an organic polymer as a binder, so as to fabricate a composite membrane; and (b) inserting one end of a sheet laminate comprising a cathode sheet and an anode sheet as well as the composite membrane into a mandrel, winding the sheet laminate around the mandrel, and then, removing the mandrel, wherein the organic/inorganic composite layer includes microfine pores capable of moderating a variation in volume during charge/discharge of a secondary battery and an interfacial friction coefficient between the composite membrane and the mandrel is not more than 0.28.
    Type: Grant
    Filed: October 8, 2008
    Date of Patent: October 28, 2014
    Assignee: LG Chem, Ltd.
    Inventors: Youngkwang Yun, Sangbaek Ryu, Jinsoo Lee, SooRyoung Kim, Byungjin Choi, Hyang Mok Lee
  • Patent number: 8753777
    Abstract: Disclosed is a secondary battery including a cathode, an anode, a membrane and an electrolyte, wherein the cathode contains a mixture of a first cathode material defined herein and a second cathode material selected from the group consisting of a second-(a) cathode material defined herein and a second-(b) cathode material defined herein, and a combination thereof, wherein a mix ratio of the two cathode materials (first cathode material:second cathode material) is 50:50 to 90:10, and the membrane is an organic/inorganic composite porous membrane including (a) a polyolefin-based membrane substrate and (b) an active layer in which one or more areas selected from the group consisting of the surface of the substrate and a portion of pores of the substrate are coated with a mixture of inorganic particles and a binder polymer, wherein the active layer has a structure in which the inorganic particles are interconnected and fixed through a binder polymer and porous structures are formed by the interstitial volume betw
    Type: Grant
    Filed: March 8, 2013
    Date of Patent: June 17, 2014
    Assignee: LG Chem, Ltd.
    Inventors: Seungeun Choi, Eungyoung Goh, Hyang Mok Lee, Heegyoung Kang, Sangbaek Ryu, Kiwoong Kim
  • Patent number: 8715856
    Abstract: Disclosed is a secondary battery including a cathode, an anode, a membrane and an electrolyte, wherein the cathode contains a mixture of a first cathode material defined herein and a second cathode material selected from the group consisting of a second-(a) cathode material defined herein and a second-(b) cathode material defined herein, and a combination thereof, wherein a mix ratio of the two cathode materials (first cathode material: second cathode material) is 50:50 to 90:10, and the membrane is an organic/inorganic composite porous membrane including (a) a polyolefin-based membrane substrate and (b) an active layer in which one or more areas selected from the group consisting of the surface of the substrate and a portion of pores of the substrate are coated with a mixture of inorganic particles and a binder polymer, wherein the active layer has a structure in which the inorganic particles are interconnected and fixed through a binder polymer and porous structures are formed by the interstitial volume bet
    Type: Grant
    Filed: September 1, 2011
    Date of Patent: May 6, 2014
    Assignee: LG Chem, Ltd.
    Inventors: Seungeun Choi, Eunyoung Goh, Hyang Mok Lee, Heegyoung Kang, Sangbaek Ryu, Kiwoong Kim
  • Publication number: 20140106212
    Abstract: Disclosed is a cathode material comprising a mixture of an oxide powder (a) defined herein and an oxide powder (b) selected from the group consisting of an oxide powder (b1) defined herein and an oxide powder (b2) defined herein and a combination thereof wherein a mix ratio of the two oxide powders (oxide powder (a): oxide powder (b)) is 50:50 to 90:10. The cathode material uses a combination of an oxide powder (a) and 50% or less of an oxide powder (b) which can exert high capacity, high cycle stability, superior storage stability and high-temperature stability, thus advantageously exhibiting high energy density and realizing high capacity batteries.
    Type: Application
    Filed: November 4, 2013
    Publication date: April 17, 2014
    Applicant: LG CHEM, LTD.
    Inventors: Seungeun CHOI, Eunyoung GOH, Hyang Mok LEE, Heegyoung KANG, Sangbaek RYU, Kiwoong KIM
  • Patent number: 8603676
    Abstract: Disclosed is a cathode material comprising a mixture of an oxide powder (a) defined herein and an oxide powder (b) selected from the group consisting of an oxide powder (b1) defined herein and an oxide powder (b2) defined herein and a combination thereof wherein a mix ratio of the two oxide powders (oxide powder (a):oxide powder (b)) is 50:50 to 90:10. The cathode material uses a combination of an oxide powder (a) and 50% or less of an oxide powder (b) which can exert high capacity, high cycle stability, superior storage stability and high-temperature stability, thus advantageously exhibiting high energy density and realizing high capacity batteries.
    Type: Grant
    Filed: September 1, 2011
    Date of Patent: December 10, 2013
    Assignee: LG Chem, Ltd.
    Inventors: Seungeun Choi, Eunyoung Goh, Hyang Mok Lee, Heegyoung Kang, Sangbaek Ryu, Kiwoong Kim
  • Publication number: 20130260200
    Abstract: Provided is a method for fabrication of a jelly-roll type electrode assembly having a cathode/separation membrane/anode laminate structure, including: (a) coating both sides of a porous substrate with organic/inorganic composite layers, each of which includes inorganic particles and an organic polymer as a binder, so as to fabricate a composite membrane; and (b) inserting one end of a sheet laminate comprising a cathode sheet and an anode sheet as well as the composite membrane into a mandrel, winding the sheet laminate around the mandrel, and then, removing the mandrel, wherein the organic/inorganic composite layer includes microfine pores capable of moderating a variation in volume during charge/discharge of a secondary battery and an interfacial friction coefficient between the composite membrane and the mandrel is not more than 0.28.
    Type: Application
    Filed: May 30, 2013
    Publication date: October 3, 2013
    Inventors: Youngkwang YUN, Sangbaek RYU, Jinsoo LEE, SooRyoung KIM, Byungjin CHOI, Hyang Mok LEE
  • Publication number: 20120225343
    Abstract: Disclosed is a cathode material comprising a mixture of an oxide powder (a) defined herein and an oxide powder (b) selected from the group consisting of an oxide powder (b1) defined herein and an oxide powder (b2) defined herein and a combination thereof wherein a mix ratio of the two oxide powders (oxide powder (a): oxide powder (b)) is 50:50 to 90:10. The cathode material uses a combination of an oxide powder (a) and 50% or less of an oxide powder (b) which can exert high capacity, high cycle stability, superior storage stability and high-temperature stability, thus advantageously exhibiting high energy density and realizing high capacity batteries.
    Type: Application
    Filed: September 1, 2011
    Publication date: September 6, 2012
    Applicant: LG CHEM, LTD.
    Inventors: Seungeun CHOI, Eunyoung GOH, Hyang Mok LEE, Heegyoung KANG, Sangbaek RYU, Kiwoong KIM
  • Publication number: 20120219840
    Abstract: Disclosed is a secondary battery including a cathode, an anode, a membrane and an electrolyte, wherein the cathode contains a mixture of a first cathode material defined herein and a second cathode material selected from the group consisting of a second-(a) cathode material defined herein and a second-(b) cathode material defined herein, and a combination thereof, wherein a mix ratio of the two cathode materials (first cathode material: second cathode material) is 50:50 to 90:10, and the membrane is an organic/inorganic composite porous membrane including (a) a polyolefin-based membrane substrate and (b) an active layer in which one or more areas selected from the group consisting of the surface of the substrate and a portion of pores of the substrate are coated with a mixture of inorganic particles and a binder polymer, wherein the active layer has a structure in which the inorganic particles are interconnected and fixed through a binder polymer and porous structures are formed by the interstitial volume bet
    Type: Application
    Filed: September 1, 2011
    Publication date: August 30, 2012
    Applicant: LG CHEM, LTD.
    Inventors: Seungeun CHOI, Eunyoung GOH, Hyang Mok LEE, Heegyoung KANG, Sangbaek RYU, Kiwoong KIM
  • Publication number: 20100285341
    Abstract: Provided is a method for fabrication of a jelly-roll type electrode assembly having a cathode/separation membrane/anode laminate structure, including: (a) coating both sides of a porous substrate with organic/inorganic composite layers, each of which includes inorganic particles and an organic polymer as a binder, so as to fabricate a composite membrane; and (b) inserting one end of a sheet laminate comprising a cathode sheet and an anode sheet as well as the composite membrane into a mandrel, winding the sheet laminate around the mandrel, and then, removing the mandrel, wherein the organic/inorganic composite layer includes microfine pores capable of moderating a variation in volume during charge/discharge of a secondary battery and an interfacial friction coefficient between the composite membrane and the mandrel is not more than 0.28.
    Type: Application
    Filed: October 8, 2008
    Publication date: November 11, 2010
    Applicant: LG CHEM,LTD.
    Inventors: Youngkwang Yun, Sangbaek Ryu, Jinsoo Lee, SooRyoung Kim, Byungjin Choi, Hyang Mok Lee