  • Publication number: 20120174713
    Abstract: A method of agglomerating a nickel laterite ore comprising the steps of: i) feeding a nickel laterite ore material to be agglomerated into an agglomeration circuit; and ii) adding a sulfuric acid containing agglomerating solution to the ore material in the agglomeration circuit to provide an agglomerated ore material, wherein the acid concentration of the agglomerating solution is between 100 to 400 g/L.
    Type: Application
    Filed: February 2, 2010
    Publication date: July 12, 2012
    Inventors: Nelson Mora, Adam Sean Moroney, Scott Thomas
  • Patent number: 8197575
    Abstract: A process for heap leaching a laterite that includes providing a primary and a secondary heap, with the primary heap comprising predominantly a nickel and cobalt containing sulfide or saprolitic type ore, and the secondary heap comprising predominantly a nickel and cobalt limonitic type ore; leaching the primary heap with a sulfuric acid solution to generate a solution that includes ferrous ions; and using the solution that includes the ferrous ion as the lixiviant to leach the secondary heap, to produce a pregnant leach solution that includes nickel, cobalt and manganese ions.
    Type: Grant
    Filed: December 24, 2008
    Date of Patent: June 12, 2012
    Assignee: BHP Billiton SSM Development Pty Ltd.
    Inventor: Adam Sean Moroney
  • Patent number: 7988938
    Abstract: A heap leach process for the recovery of nickel and cobalt from a lateritic ore, said process including the steps of leaching and/or agglomerating the ore with a lixiviant that includes ferrous ions, wherein the lixiviant is able to liberate cobalt from the cobalt containing minerals within the ore in preference to nickel, to produce a cobalt rich pregnant leach solution relatively free of nickel.
    Type: Grant
    Filed: December 24, 2008
    Date of Patent: August 2, 2011
    Assignee: BHP Billiton SSM Development Pty Ltd.
    Inventors: Eric Girvan Roche, Adam Sean Moroney, Houyuan Liu
  • Publication number: 20110056332
    Abstract: A process for heap leaching a laterite or said process including the steps of: a) providing a primary and a secondary heap, said primary heap comprising predominantly a nickel and cobalt containing sulfide or saprolitic type ore, and said secondary heap comprising predominantly a nickel and cobalt limonitic type ore; b) leaching the primary heap with a sulfuric acid solution to generate a solution that includes ferrous ions; and c) using said solution that includes the ferrous ion as the lixiviant to leach the secondary heap, to produce a pregnant leach solution that includes nickel, cobalt and manganese ions.
    Type: Application
    Filed: December 24, 2008
    Publication date: March 10, 2011
    Inventor: Adam Sean Moroney
  • Publication number: 20100296988
    Abstract: A heap leach process for the recovery of nickel and cobalt from a lateritic ore, said process including the steps of leaching and/or agglomerating the ore with a lixiviant that includes ferrous ions, wherein the lixiviant is able to liberate cobalt from the cobalt containing minerals within the ore in preference to nickel, to produce a cobalt rich pregnant leach solution relatively free of nickel.
    Type: Application
    Filed: December 24, 2008
    Publication date: November 25, 2010
    Applicant: BHP BILLITON SSM DEVELOPMENT PTY LTD
    Inventors: Eric Girvan Roche, Adam Sean Moroney, Houyuan Liu
  • Publication number: 20100282024
    Abstract: A process for the recovery of nickel and/or cobalt from a lateritic ore by heap leaching, the process including the steps of: a) forming one or more heaps from a lateritic ore body wherein that lateritic ore body includes a blend of both limonitic and saprolitic type ores; b) leaching the one or more heaps with a leach solution; and c) recovering the nickel and/or cobalt from the resultant heap leachate.
    Type: Application
    Filed: September 12, 2008
    Publication date: November 11, 2010
    Applicant: BHP BILLITON SSM DEVELOPMENT PTY. LTD
    Inventors: Adam Sean Moroney, Omar Yesid Caceres Hernandez, Houyuan Liu
  • Patent number: 7601314
    Abstract: A process for the recovery of nickel and/or cobalt from an impure nickel, cobalt or mixed nickel/cobalt material including the steps of: a) providing a nickel, cobalt or mixed nickel/cobalt material; and b) contacting the nickel, cobalt or mixed nickel/cobalt material with a feed ammoniacal ammonium carbonate solution and a reductant in a leach step.
    Type: Grant
    Filed: April 8, 2004
    Date of Patent: October 13, 2009
    Assignee: BHP Billiton SSM Technology Pty Ltd
    Inventors: Peter Allan Anderson, Mark Fisher, John Ernest Fittock, Victoria Margaret Hultgren, Erin Maree Jones, Robert Bruce Messenger, Adam Sean Moroney
  • Patent number: D810610
    Type: Grant
    Filed: August 11, 2016
    Date of Patent: February 20, 2018
    Assignee: SENTIENT JEWELRY, LLC
    Inventors: Maria Corcoran, Sean Moroney