  • Patent number: 9926259
    Abstract: The present invention relates to a catalyst for fixed bed aniline rectification residue recycling and preparation method thereof. Based on the total weight of the catalyst, the catalyst comprises the following components in percentage by weight: 5-40% of an active component, 2-30% of a first cocatalyst component, 10-30% of a second cocatalyst component and the balance of carrier, wherein the active component is NiO; the first cocatalyst component is one or more of Fe, Mo, Cr or Co oxide; and the second cocatalyst component is one or more of La, Zr, Y or Ce oxide. The catalyst is prepared through co-precipitation. The catalyst shows high activity and stability in the waste liquid treatment process, and can still maintain high rectification residue cracking rate after reaction of 200 hours.
    Type: Grant
    Filed: September 29, 2017
    Date of Patent: March 27, 2018
    Assignee: Wanhua Chemical Group Co., Ltd.
    Inventors: Hua Mei, Hao Chen, Dewei Yu, Congying Zhang, Hui Wang, Yuan Li, Zhongying Chen, Zilin Ni, Qingmei Jiang, Shanjian Cao, Zaigang Yang, Jun Qu, Jinhong Song, Bingbo Hu
  • Publication number: 20180065916
    Abstract: The present invention relates to a catalyst for fixed bed aniline rectification residue recycling and preparation method thereof. Based on the total weight of the catalyst, the catalyst comprises the following components in percentage by weight: 5-40% of an active component, 2-30% of a first cocatalyst component, 10-30% of a second cocatalyst component and the balance of carrier, wherein the active component is NiO; the first cocatalyst component is one or more of Fe, Mo, Cr or Co oxide; and the second cocatalyst component is one or more of La, Zr, Y or Ce oxide. The catalyst is prepared through co-precipitation. The catalyst shows high activity and stability in the waste liquid treatment process, and can still maintain high rectification residue cracking rate after reaction of 200 hours.
    Type: Application
    Filed: September 29, 2017
    Publication date: March 8, 2018
    Inventors: Hua Mei, Hao Chen, Dewei Yu, Congying Zhang, Hui Wang, Yuan Li, Zhongying Chen, Zilin Ni, Qingmei Jiang, Shanjian Cao, Zaigang Yang, Jun Qu, Jinhong Song, Bingbo Hu
  • Publication number: 20160207876
    Abstract: The present invention relates to a catalyst for fixed bed aniline rectification residue recycling and preparation method thereof. Based on the total weight of the catalyst, the catalyst comprises the following components in percentage by weight: 5-40% of an active component, 2-30% of a first cocatalyst component, 10-30% of a second cocatalyst component and the balance of carrier, wherein the active component is NiO; the first cocatalyst component is one or more of Fe, Mo, Cr or Co oxide; and the second cocatalyst component is one or more of La, Zr, Y or Ce oxide. The catalyst is prepared through co-precipitation. The catalyst shows high activity and stability in the waste liquid treatment process, and can still maintain high rectification residue cracking rate after reaction of 200 hours.
    Type: Application
    Filed: March 7, 2014
    Publication date: July 21, 2016
    Inventors: Hua Mei, Hao CHEN, Dewei YU, Congying ZHANG, Hui WANG, Yuan LI, Zhongying CHEN, Zilin NI, Qingmei JIANG, Shanjian CAO, Zaigang YANG, Jun QU, Jinhong SONG, Bingbo HU