Publication number: 20150183967Abstract: Provided is a cellulose ester-based resin composition having excellent processability, resistance to coloration caused by processing and flame retardancy. Also provided is a molded article having excellent color tone and flame retardancy. The cellulose ester-based resin composition of the present invention is characterized by comprising 1 to 50 parts by mass of a phosphate represented by the following Formula (1) with respect to 100 parts by mass of a cellulose ester-based resin: (wherein, R1 and R2 each independently represent a hydrogen atom or a methyl group; and n represents an integer of 1 to 5).Type: ApplicationFiled: June 5, 2013Publication date: July 2, 2015Applicant: ADEKA CORPORATIONInventors: Takashi Ayabe, Yuki Endo, Tetsuya Seguchi
-
Publication number: 20150158996Abstract: Provided is a masterbatch in which blocking in a masterbatch of a hindered amine compound and a benzoate compound, which is caused by long-term storage under a high-temperature environment, is improved.Type: ApplicationFiled: July 3, 2013Publication date: June 11, 2015Applicant: ADEKA CORPORATIONInventors: Takashi Ayabe, Kenji Yamashita
-
Publication number: 20150152248Abstract: Provided is a method of producing a nucleator masterbatch, by which a nucleator masterbatch capable of improving the transparency and the physical properties of an olefin resin can be produced. This method is a method of producing a masterbatch in which a nucleator is blended in an olefin polymer, the method being characterized by comprising the step of polymerizing an olefin monomer with incorporation of a nucleator component, which is dissolved in an organoaluminum compound or in an organoaluminum compound and an organic solvent, before or during polymerization of the olefin monomer such that the nucleator component is blended in an amount of 0.05 to 20 parts by mass with respect to 100 parts by mass of the olefin polymer obtained by the polymerization of the olefin monomer.Type: ApplicationFiled: May 30, 2013Publication date: June 4, 2015Applicant: ADEKA CORPORATIONInventors: Naoshi Kawamoto, Takashi Ayabe, Atsushi Sakai, Tetsuya Seguchi
-
Publication number: 20150119513Abstract: The present invention provides a stabilizer composition comprising a monoester and diester of alkylmercapto carboxylic acid of bisphenol sulfide, which is capable of maintaining good ease of handling without causing precipitation of solids even in low temperature environments.Type: ApplicationFiled: May 23, 2013Publication date: April 30, 2015Applicant: ADEKA CORPORATIONInventors: Naoshi Kawamoto, Yoshinori Negishi, Takashi Ayabe, Tsuyoshi Urushihara, Tomomasa Teduka, Shingo Yamada
-
Publication number: 20140378586Abstract: Provided is an additive masterbatch having excellent storage stability (agglomeration resistance), which also has reduced surface tackiness despite comprising a low-melting-point resin additive at a high concentration. The resin additive masterbatch of the present invention is characterized by comprising, with respect to 100 parts by mass of (A) a polyolefin resin, 65 to 300 parts by mass of (B) a resin additive having a melting point of not higher than 80° C.; and 0.8 to 24 parts by mass of (C) a benzotriazole-based ultraviolet absorber.Type: ApplicationFiled: July 31, 2012Publication date: December 25, 2014Applicant: ADEKA CORPORATIONInventors: Takashi Ayabe, Kenji Yamashita, Naoki Yamamoto
-
Publication number: 20140275414Abstract: Provided are a recycling method for industrially, simply and effectively recycling a phenolic body from a phenolic antioxidant which is masked by an organoaluminum compound and contained in an olefin polymer obtained by supplying the masked phenolic antioxidant upon polymerization; and an olefin polymer obtained by this method. In a method for recycling a phenolic antioxidant wherein a phenolic antioxidant which is masked by an organoaluminum compound and contained in an olefin polymer obtained by supplying the masked phenolic antioxidant upon polymerization is recycled to a phenolic body, a nitrogen gas comprising water and/or a proton donor at a volume ratio of 1.0×10?6 to 2.5×10?2 with respect to 1 volume of nitrogen is brought into contact with the olefin polymer.Type: ApplicationFiled: June 2, 2014Publication date: September 18, 2014Applicant: ADEKA CORPORATIONInventors: Naoshi KAWAMOTO, Takashi AYABE, Tsuyoshi URUSHIHARA, Kohei OKAMOTO, Tetsuya SEGUCHI
-
Publication number: 20130023611Abstract: Hindered amines represented by the general formula (I): (wherein R is an alkyl or hydroxyalkyl group having 1 to 30 carbon atoms or alkenyl having 2 to 30 carbon atoms; n is an integer of 1 to 4; when n is 1, R1 is alkyl having 1 to 22 carbon atoms, alkenyl having 2 to 22 carbon atoms, or a group represented by the general formula (III): (R is as defined above), while when n is 2 to 4, R1 is an n-valent organic group having 2 to 20 carbon atoms). When added to synthetic resins or coating materials, the amines can impart long-period stabilizing effect to the resins or the materials and exhibit excellent resistance to extraction with acid rain or chemicals.Type: ApplicationFiled: September 13, 2012Publication date: January 24, 2013Applicant: ADEKA CORPORATIONInventors: Yoshinori NEGISHI, Takashi AYABE, Etsuo TOBITA
-
Patent number: 8329787Abstract: Hindered amines represented by the general formula (I): (wherein R is an alkyl or hydroxyalkyl group having 1 to 30 carbon atoms or alkenyl having 2 to 30 carbon atoms; n is an integer of 1 to 4; when n is 1, R1 is alkyl having 1 to 22 carbon atoms, alkenyl having 2 to 22 carbon atoms, or a group represented by the general formula (III): (R is as defined above), while when n is 2 to 4, R1 is an n-valent organic group having 2 to 20 carbon atoms). When added to synthetic resins or coating materials, the amines can impart long-period stabilizing effect to the resins or the materials and exhibit excellent resistance to extraction with acid rain or chemicals.Type: GrantFiled: April 2, 2010Date of Patent: December 11, 2012Assignee: Adeka CorporationInventors: Yoshinori Negishi, Takashi Ayabe, Etsuo Tobita
-
Publication number: 20120149838Abstract: Provided are a recycling method for industrially, simply and effectively recycling a phenolic body from a phenolic antioxidant which is masked by an organoaluminum compound and contained in an olefin polymer obtained by supplying the masked phenolic antioxidant upon polymerization; and an olefin polymer obtained by this method. In a method for recycling a phenolic antioxidant wherein a phenolic antioxidant which is masked by an organoaluminum compound and contained in an olefin polymer obtained by supplying the masked phenolic antioxidant upon polymerization is recycled to a phenolic body, a nitrogen gas comprising water and/or a proton donor at a volume ratio of 1.0×10?6 to 2.5×10?2 with respect to 1 volume of nitrogen is brought into contact with the olefin polymer.Type: ApplicationFiled: September 1, 2010Publication date: June 14, 2012Applicant: ADEKA CORPORATIONInventors: Naoshi Kawamoto, Takashi Ayabe, Tsuyoshi Urushihara, Kohei Okamoto, Tetsuya Seguchi
-
Publication number: 20120022212Abstract: Provided is a polyolefin-based resin composition having sufficient stabilizing effect and excellent cost performance. The polyolefin-based resin composition according to the present invention comprises a polyolefin-based resin obtained by polymerization of an olefin-based monomer with an addition of a phenolic antioxidant represented by the following Formula (I): (wherein, R represents a C1-C30 alkyl group or C2-C30 alkylene group which is optionally branched and/or optionally has a cycloalkyl group, a C3-C12 cycloalkyl group which is optionally substituted or a C6-C18 aryl group which is optionally substituted), which phenolic antioxidant is masked with an organic aluminum compound, and a phosphorus-based antioxidant to a catalyst system or polymerization system before or during the polymerization of the olefin-based monomer, in which polyolefin-based resin composition, the phenolic antioxidant represented by the Formula (I) and the phosphorus-based antioxidant are added in an amount of 0.001 to 0.Type: ApplicationFiled: November 13, 2009Publication date: January 26, 2012Inventors: Takashi Ayabe, Kohei Okamoto, Tetsuya Seguchi, Naoshi Kawamoto
-
Publication number: 20110288216Abstract: The present invention provides a stabilized polyolefin-based resin composition for use in food items, medical services and water service pipes, which has superior non-migratory and hygienic properties.Type: ApplicationFiled: November 13, 2009Publication date: November 24, 2011Inventors: Takashi Ayabe, Kohei Okamoto, Tetsuya Seguchi, Naoshi Kawamoto
-
Publication number: 20110065876Abstract: The invention relates to an aluminum phenoxide compound produced without using aromatic solvent and represented by general formula (I) below. A stabilized polymer can be produced by adding the aluminum phenoxide compound to a catalyst system or a polymerization system before or during polymerization. In the formula, A represents an alkyl group having 2 to 6 carbon atoms, a halogen atom, or methylaminoxane; B represents a hexadecyl group, a heptadecyl group, or an octadecyl group; l, m, and n represent numbers that satisfy expressions m?1, l?1, m+n=3, and l+n=3; when m or l exceeds 1, then A may be different from each other; and when the number of moles of aluminum is expressed as “t”, then t/n?1.3.Type: ApplicationFiled: May 25, 2009Publication date: March 17, 2011Applicant: ADEKA CORPORATIONInventors: Kohei Okamoto, Naoshi Kawamoto, Takashi Ayabe
-
Publication number: 20100305327Abstract: The following compound, inhibitor, and composition are provided: a compound having low volatility, high nitroxyl group concentration, and high polymerization inhibitory activity; a polymerization inhibitor using the compound; and a polymerization inhibitor composition using the compound.Type: ApplicationFiled: December 6, 2006Publication date: December 2, 2010Applicant: ADEKA CORPORATIONInventors: Yoshinori Negishi, Etsuo Tobita, Takashi Ayabe
-
Patent number: 7842744Abstract: The present invention provides an optical film, which is excellent in ultraviolet absorption capability at 380 nm with little bleed-out, comprising a resin containing a triazine compound represented by the following general formula (I). (In the formula, R1-R6 may be a hydrogen atom; hydroxyl group; or an organic group selected from among an alkyl group, alkoxy group, dialkyl amino group, alkyl carbonyloxy group, aryl group, arylated alkyl group, aryloxy group, arylated alkyloxy group and an aryl carbonyloxy group having 18 or less carbon atoms, independently. However, the alkyl part of these organic groups may be substituted by a hydroxyl group, halogen atom, cyano group or nitro group, interrupted by an oxygen atom, sulfur atom, carbonyl group, ester group, amide group or imino group, or have a double bond, and these substitutions, interruptions and double bonds may be combined).Type: GrantFiled: March 10, 2009Date of Patent: November 30, 2010Assignee: Adeka CorporationInventors: Yoshinori Negishi, Shinichi Ishikawa, Etsuo Tobita, Takashi Ayabe
-
Publication number: 20100190898Abstract: Hindered amines represented by the general formula (I): (wherein R is an alkyl or hydroxyalkyl group having 1 to 30 carbon atoms or alkenyl having 2 to 30 carbon atoms; n is an integer of 1 to 4; when n is 1, R1 is alkyl having 1 to 22 carbon atoms, alkenyl having 2 to 22 carbon atoms, or a group represented by the general formula (III): (R is as defined above), while when n is 2 to 4, R1 is an n-valent organic group having 2 to 20 carbon atoms). When added to synthetic resins or coating materials, the amines can impart long-period stabilizing effect to the resins or the materials and exhibit excellent resistance to extraction with acid rain or chemicals.Type: ApplicationFiled: April 2, 2010Publication date: July 29, 2010Inventors: Yoshinori Negishi, Takashi Ayabe, Etsuo Tobita
-
Publication number: 20100174015Abstract: [Object] To provide a polymeric material composition having high heat resistance, excellent compatibility, and greatly improved weatherability. [Solving Means] A polymeric material composition containing: a polymeric material and a triazine compound having the general formula (I): wherein R1 to R3 denote an alkyl group, a cycloalkyl group, an alkenyl group, an aryl group, an alkylaryl group, or an arylalkyl group, these groups being optionally substituted by a hydroxy group, a halogen atom, a cyano group, a nitro group, an alkyl group, or an alkoxy group, and/or being optionally interrupted by an oxygen atom, a sulfur atom, a carbonyl group, an ester group, an amide group, or an imino group; R4 to R6 denote an alkyl group or an alkenyl group; and R7 to R9 denote a hydrogen atom, a halogen atom, an alkyl group, or an alkenyl group.Type: ApplicationFiled: March 27, 2007Publication date: July 8, 2010Applicant: Adeka CorporationInventors: Yoshinori Negishi, Takashi Ayabe, Masato Suzuki, Etsuo Tobita
-
Publication number: 20090258976Abstract: The present invention provides an optical film, which is excellent in ultraviolet absorption capability at 380 nm with little bleed-out, comprising a resin containing a triazine compound represented by the following general formula (I). (In the formula, R1-R6 may be a hydrogen atom; hydroxyl group; or an organic group selected from among an alkyl group, alkoxy group, dialkyl amino group, alkyl carbonyloxy group, aryl group, arylated alkyl group, aryloxy group, arylated alkyloxy group and an aryl carbonyloxy group having 18 or less carbon atoms, independently. However, the alkyl part of these organic groups may be substituted by a hydroxyl group, halogen atom, cyano group or nitro group, interrupted by an oxygen atom, sulfur atom, carbonyl group, ester group, amide group or imino group, or have a double bond, and these substitutions, interruptions and double bonds may be combined).Type: ApplicationFiled: March 10, 2009Publication date: October 15, 2009Inventors: Yoshinori NEGISHI, Shinichi Ishikawa, Etsuo Tobita, Takashi Ayabe
-
Patent number: 7553892Abstract: The present invention provides an optical film, which is excellent in ultraviolet absorption capability at 380 nm with little bleed-out, comprising a resin containing a triazine compound represented by the following general formula (I). (In the formula, R1-R6 may be a hydrogen atom; hydroxyl group; or an organic group selected from among an alkyl group, alkoxy group, dialkyl amino group, alkyl carbonyloxy group, aryl group, arylated alkyl group, aryloxy group, arylated alkyloxy group and an aryl carbonyloxy group having 18 or less carbon atoms, independently. However, the alkyl part of these organic groups may be substituted by a hydroxyl group, halogen atom, cyano group or nitro group, interrupted by an oxygen atom, sulfur atom, carbonyl group, ester group, amide group or imino group, or have a double bond, and these substitutions, interruptions and double bonds may be combined).Type: GrantFiled: April 26, 2005Date of Patent: June 30, 2009Assignee: Adeka CorporationInventors: Yoshinori Negishi, Shinichi Ishikawa, Etsuo Tobita, Takashi Ayabe
-
Publication number: 20090111699Abstract: Hindered amines represented by the general formula (I): (wherein R is an alkyl or hydroxyalkyl group having 1 to 30 carbon atoms or alkenyl having 2 to 30 carbon atoms; n is an integer of 1 to 4; when n is 1, R1 is alkyl having 1 to 22 carbon atoms, alkenyl having 2 to 22 carbon atoms, or a group represented by the general formula (III): (R is as defined above), while when n is 2 to 4, R1 is an n-valent organic group having 2 to 20 carbon atoms). When added to synthetic resins or coating materials, the amines can impart long-period stabilizing effect to the resins or the materials and exhibit excellent resistance to extraction with acid rain or chemicals.Type: ApplicationFiled: February 28, 2005Publication date: April 30, 2009Applicant: ADEKA CORPORATIONInventors: Yoshinori Negishi, Takashi Ayabe, Etsuo Tobita
-
Publication number: 20070215845Abstract: The present invention provides an optical film, which is excellent in ultraviolet absorption capability at 380 nm with little bleed-out, comprising a resin containing a triazine compound represented by the following general formula (I). (In the formula, R1-R6 may be a hydrogen atom; hydroxyl group; or an organic group selected from among an alkyl group, alkoxy group, dialkyl amino group, alkyl carbonyloxy group, aryl group, arylated alkyl group, aryloxy group, arylated alkyloxy group and an aryl carbonyloxy group having 18 or less carbon atoms, independently. However, the alkyl part of these organic groups may be substituted by a hydroxyl group, halogen atom, cyano group or nitro group, interrupted by an oxygen atom, sulfur atom, carbonyl group, ester group, amide group or imino group, or have a double bond, and these substitutions, interruptions and double bonds may be combined).Type: ApplicationFiled: April 26, 2005Publication date: September 20, 2007Inventors: Yoshinori Negishi, Shinichi Ishikawa, Etsuo Tobita, Takashi Ayabe