Patents by Inventor Yoshifumi Araki

Yoshifumi Araki has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Publication number: 20170002190
    Abstract: A block copolymer composition including: 10% by mass or more and 90% by mass or less of a component (a), and 10% by mass or more and 90% by mass or less of a component (b), wherein the component (a) is a block copolymer containing a polymer block (A) primarily including a vinyl aromatic monomer unit and a polymer block (B) primarily including a conjugated diene monomer unit, wherein the block copolymer has a weight average molecular weight of 30,000 or higher and 150,000 or lower; and the component (b) is a block copolymer containing a polymer block (A) primarily including a vinyl aromatic monomer unit and a polymer block (B) primarily including a conjugated diene monomer unit.
    Type: Application
    Filed: January 22, 2015
    Publication date: January 5, 2017
    Applicants: Asahi Kasei Kabushiki Kaisha, Japan Elastomer Co., Ltd.
    Inventors: Takahiro Hisasue, Shigeo Nakajima, Yoshifumi Araki, Yukinori Nakamichi
  • Patent number: 9522393
    Abstract: A catalyst composition for hydrogenation including (A) to (D), in which a mass ratio (D)/(A) is 0.01 to 2.00. (A): a titanocene compound represented by following formula (1), (wherein R5 and R6 are selected from the group consisting of hydrogen, a hydrocarbon group having 1 to 12 carbon atoms, an aryloxy group, an alkoxy group, a halogen group, and a carbonyl group, and R1 and R2 are selected from hydrogen and a hydrocarbon group having 1 to 12 carbon atoms) (B): a compound containing an element selected from Li, Na, K, Mg, Zn, Al, and Ca, (C): an unsaturated polymer having a fraction of an olefinic unsaturated double bond content of side chains based on a total olefinic unsaturated double bond content of 0.25 to 1.0, and (D): a polar compound.
    Type: Grant
    Filed: September 12, 2013
    Date of Patent: December 20, 2016
    Assignee: Asahi Kasei Chemicals Corporation
    Inventors: Yoshifumi Araki, Eiji Sasaya, Katsunori Nitta
  • Publication number: 20160333132
    Abstract: The polymer according to the present invention is a polymer containing a conjugated diene monomer unit and a vinyl aromatic monomer unit, wherein the polymer has a polymer block (A) containing the vinyl aromatic monomer unit as a main component and a polymer block (B) containing the conjugated diene monomer unit and the vinyl aromatic monomer unit, a content of the polymer block (A) is 10% by mass or more and 40% by mass or less, a bulk density of the polymer is 0.05 g/mL or more and 0.45 g/mL or less, and a specific surface area of the polymer is 0.10 m2/g or more and 0.60 m2/g or less.
    Type: Application
    Filed: January 16, 2015
    Publication date: November 17, 2016
    Applicant: Asahi Kasei Kabushiki Kaisha
    Inventors: Takayuki Shiromoto, Shigeo Nakajima, Yoshifumi Araki, Nobuaki Kubo, Takuya Suzuki
  • Publication number: 20160333235
    Abstract: Disclosure provides a block copolymer composition having 20% by mass or more and 90% by mass or less of a component (A) and 10% by mass or more and 80% by mass or less of a component (B), wherein the component (A) is a block copolymer having a polymer block mainly comprising a vinyl aromatic monomer unit and a polymer block mainly comprising a conjugated diene monomer unit, and having a weight-average molecular weight of 30,000 or higher and 190,000 or lower; and the component (B) is a block copolymer having a polymer block mainly comprising a vinyl aromatic monomer unit and a polymer block mainly comprising a conjugated diene monomer unit, and having a weight-average molecular weight of 60,000 or higher and 500,000 or lower.
    Type: Application
    Filed: January 22, 2015
    Publication date: November 17, 2016
    Applicants: Asahi Kasei Kabushiki Kaisha, Japan Elastomer Co., Ltd.
    Inventors: Kosuke Nakatani, Yoshifumi Araki, Kenta Shibuya, Takahiro Hisasue, Kazuo Moritou
  • Patent number: 9493623
    Abstract: The present invention provides a crosslinked foam having an excellent balance of various physical properties in terms of lightness, flexibility, permanent compression set, tear strength, impact resilience, and molding stability; a shoe midsole; and a crosslinkable and foamable composition that provides the crosslinked foam and shoe midsole. A crosslinkable and foamable composition comprising (A) an ethylene-based copolymer; (B) a copolymer comprising a vinyl aromatic monomer unit and an unsaturated bond-containing a conjugated diene monomer unit; (C) an organic peroxide; and (D) a foaming agent; a mass ratio of the component (A) to the component (B), (A/B), being from 97/3 to 50/50; and the component (B) comprising 5 mass % or more and 80 mass % or less of the vinyl aromatic monomer unit, and 5 mass % or more and 55 mass % or less of the conjugated diene monomer unit.
    Type: Grant
    Filed: December 21, 2009
    Date of Patent: November 15, 2016
    Assignee: ASAHI KASEI CHEMICALS CORPORATION
    Inventors: Daisuke Shimizu, Yoshifumi Araki, Katsumi Suzuki, Yasuhiro Kusanose, Mika Horiuchi
  • Patent number: 9365706
    Abstract: A crosslinked composition is obtained by crosslinking a composition, containing: 1 to 99 parts by mass of a vinyl aromatic copolymer rubber (I) comprising 5 to 70% by mass of a vinyl aromatic monomer unit and 0.1 to 30% by mass of a conjugated diene monomer unit and having one or more tan ? peak temperatures between 75° C. and 125° C.; 99 to 1 parts by mass of an ethylenic copolymer rubber (II); 10 to 100 parts by mass of an olefinic resin (III) based on 100 parts by mass of a total amount of the vinyl aromatic copolymer rubber (I) and the ethylenic copolymer rubber (II); and 0.01 to 50 parts by mass of a crosslinking agent (IV) based on 100 parts by mass of the total amount of the vinyl aromatic copolymer rubber (I) and the ethylenic copolymer rubber (II).
    Type: Grant
    Filed: September 14, 2012
    Date of Patent: June 14, 2016
    Assignee: Asahi Kasei Chemicals Corporation
    Inventors: Daisuke Shimizu, Yoshifumi Araki, Katsumi Suzuki
  • Publication number: 20150353669
    Abstract: A method for producing a polymer has: a polymerization step of polymerizing at least a conjugated diene monomer in a hydrocarbon solvent using an organolithium compound as a polymerization initiator, and obtaining a polymer; and, following steps (1) to (4), successively performing after the polymerization step: (1) a step of mixing an acid and water of 20 to 300 parts by mass into the solution containing the polymer of 100 parts by mass, (2) a step of adjusting an amount of the water to 10 parts by mass or less based on 100 parts by mass of the solution containing the polymer, (3) a step of adding a carbon oxide gas and/or a compound to be decarboxylated to the solution containing the polymer, and (4) a step of removing a solvent from the solution containing the polymer until a concentration of the polymer reaches 95 mass % or more.
    Type: Application
    Filed: January 8, 2014
    Publication date: December 10, 2015
    Applicant: Asahi Kasei Chemicals Corporation
    Inventors: Yoshifumi Araki, Eiji Sasaya, Takuya Suzuki
  • Publication number: 20150298112
    Abstract: A method for producing a catalyst composition for hydrogenation, wherein: (A): a titanocene compound represented by following general formula (1): wherein R5 and R6 represent a group selected from the group consisting of hydrogen, a hydrocarbon group having 1 to 12 carbon atoms, an aryloxy group, an alkoxy group, a halogen group and a carbonyl group, and may be the same or different, and R1 and R2 represent a group selected from the group consisting of hydrogen and a hydrocarbon group having 1 to 12 carbon atoms, and may be the same or different, provided that R1 and R2 represent are not all hydrogens or all hydrocarbon groups having 1 to 12 carbon atoms; (B): a compound containing at least one element selected from the group consisting of elements Li, Na, K, Mg, Zn, Al, and Ca; and (C): an unsaturated compound are used, and the method has: a force application step of applying a shearing force at a shearing rate of 1000 (1/s) or more to at least component (A); and a step of mixing components (A
    Type: Application
    Filed: October 22, 2013
    Publication date: October 22, 2015
    Applicant: Asahi Kasei Chemicals Corporation
    Inventors: Yoshifumi ARAKI, Eiji SASAYA, Katsunori NITTA
  • Publication number: 20150273458
    Abstract: A catalyst composition for hydrogenation including (A) to (D), in which a mass ratio (D)/(A) is 0.01 to 2.00. (A): a titanocene compound represented by following formula (1), (wherein R5 and R6 are selected from the group consisting of hydrogen, a hydrocarbon group having 1 to 12 carbon atoms, an aryloxy group, an alkoxy group, a halogen group, and a carbonyl group, and R1 and R2 are selected from hydrogen and a hydrocarbon group having 1 to 12 carbon atoms) (B): a compound containing an element selected from Li, Na, K, Mg, Zn, Al, and Ca, (C): an unsaturated polymer having a fraction of an olefinic unsaturated double bond content of side chains based on a total olefinic unsaturated double bond content of 0.25 to 1.0, and (D): a polar compound.
    Type: Application
    Filed: September 12, 2013
    Publication date: October 1, 2015
    Applicant: Asahi Kasei Chemicals Corporation
    Inventors: Yoshifumi Araki, Eiji Sasaya, Katsunori Nitta
  • Publication number: 20150273459
    Abstract: A catalyst composition for hydrogenation including (A) to (D), in which a mass ratio ((C)/(A)) is 0.1 to 4.0 and a mass ratio ((D)/(A)) is 0.01 to 1.00, (A): a titanocene compound represented by formula (1), (wherein R5 and R6 are any group selected from hydrogen, a hydrocarbon group having 1 to 12 carbon atoms, an aryloxy group, an alkoxy group, a halogen group, and a carbonyl group. R1 and R2 are any group selected from the group consisting of hydrogen and a hydrocarbon group having 1 to 12 carbon atoms, and R1 and R2 are not all hydrogen atoms or all a hydrocarbon group having 1 to 12 carbon atoms), (B): a reductant formed from a compound containing an element selected from the elements Li, Na, K, Mg, Zn, Al, and Ca, (C): an unsaturated compound having a molecular weight of 400 or less, and (D): a polar compound.
    Type: Application
    Filed: September 12, 2013
    Publication date: October 1, 2015
    Applicant: Asahi Kasei Chemicals Corporation
    Inventors: Yoshifumi Araki, Eiji Sasaya, Katsunori Nitta
  • Patent number: 9139722
    Abstract: There are provided a polypropylene-based resin composition having excellent impact resistance, tensile elongation at break and rigidity, a molded article thereof, and an automobile interior or exterior material using the same. The polypropylene-based resin composition contains 50 to 90% by mass of a polypropylene-based polymer (A), 5 to 50% by mass of an ethylene-?-olefin copolymer rubber (B), and 0.1 to 5% by mass of a copolymer (C) primarily comprising a vinyl aromatic monomer unit and an alkylene monomer unit, wherein a content of an ?-olefin monomer unit in all alkylene monomers is 45 mol % or more.
    Type: Grant
    Filed: March 12, 2010
    Date of Patent: September 22, 2015
    Assignee: ASAHI KASEI CHEMICALS CORPORATION
    Inventors: Yoshifumi Araki, Katsunori Nitta, Takashi Sato
  • Publication number: 20140357798
    Abstract: A crosslinked composition is obtained by crosslinking a composition, containing: 1 to 99 parts by mass of a vinyl aromatic copolymer rubber (I) comprising 5 to 70% by mass of a vinyl aromatic monomer unit and 0.1 to 30% by mass of a conjugated diene monomer unit and having one or more tan ? peak temperatures between 75° C. and 125° C.; 99 to 1 parts by mass of an ethylenic copolymer rubber (II); 10 to 100 parts by mass of an olefinic resin (III) based on 100 parts by mass of a total amount of the vinyl aromatic copolymer rubber (I) and the ethylenic copolymer rubber (II); and 0.01 to 50 parts by mass of a crosslinking agent (IV) based on 100 parts by mass of the total amount of the vinyl aromatic copolymer rubber (I) and the ethylenic copolymer rubber (II).
    Type: Application
    Filed: September 14, 2012
    Publication date: December 4, 2014
    Applicant: ASAHI KASEI CHEMICALS CORPORATION
    Inventors: Daisuke Shimizu, Yoshifumi Araki, Katsumi Suzuki
  • Patent number: 8901214
    Abstract: The present invention provides a resin composition that simultaneously (1) supports high productivities, (2) is resistant to bleed out by the flame retardant present in the composition, (3) is resistant to migration of its components to another resin, (4) exhibits a high flame retardancy, and (5) exhibits high flexibility. The resin composition includes components (A) a polyphenylene ether, (B) a hydrogenated copolymer, (C) a styrene resin and/or olefin resin, and (D) a metal phosphinate, wherein the component (B) includes (B1) a polymer block principally comprising an aromatic vinyl monomer unit, and (B2) a hydrogenated copolymer block principally comprising an aromatic vinyl monomer unit and a conjugated diene monomer unit, and a content of the aromatic vinyl monomer unit in the (B2) is 20 to 95% by weight, and a content of the aromatic vinyl monomer unit in the (B) is 35 to 80% by weight.
    Type: Grant
    Filed: September 23, 2011
    Date of Patent: December 2, 2014
    Assignee: Asahi Kasei Chemicals Corporation
    Inventors: Yoshifumi Araki, Takashi Sato, Takahiro Hisasue
  • Patent number: 8901222
    Abstract: The polyphenylene ether according to the present invention includes 5 to 20% by mass of a component having a molecular weight of 50,000 or more and 12 to 30% by mass of a component having a molecular weight of 8,000 or less. The resin composition according to the present invention includes the polyphenylene ether (a) and a hydrogenated block copolymer (b) prepared by hydrogenating a block copolymer including at least two polymer blocks A having a vinyl aromatic compound and at least one polymer block B having a conjugated diene compound, wherein the number average molecular weight (Mnb) of the hydrogenated block copolymer is 100,000 or less, and the number average molecular weight (MnbA) of at least one polymer block of the polymer blocks A is 8,000 or more.
    Type: Grant
    Filed: October 13, 2010
    Date of Patent: December 2, 2014
    Assignee: Asahi Kasei Chemicals Corporation
    Inventors: Shunichiro I, Yoshikuni Akiyama, Hiroshi Kamo, Yoshifumi Araki, Toru Yamaguchi, Tomohiro Kondo
  • Patent number: 8865811
    Abstract: The polyphenylene ether according to the present invention includes 5 to 20% by mass of a component having a molecular weight of 50,000 or more and 12 to 30% by mass of a component having a molecular weight of 8,000 or less. The resin composition according to the present invention includes the polyphenylene ether (a) and a hydrogenated block copolymer (b) prepared by hydrogenating a block copolymer including at least two polymer blocks A having a vinyl aromatic compound and at least one polymer block B having a conjugated diene compound, wherein the number average molecular weight (Mnb) of the hydrogenated block copolymer is 100,000 or less, and the number average molecular weight (MnbA) of at least one polymer block of the polymer blocks A is 8,000 or more.
    Type: Grant
    Filed: October 13, 2010
    Date of Patent: October 21, 2014
    Assignee: Asahi Kasei Chemicals Corporation
    Inventors: Shunichiro I, Yoshikuni Akiyama, Hiroshi Kamo, Yoshifumi Araki, Toru Yamaguchi, Tomohiro Kondo
  • Patent number: 8865804
    Abstract: The present invention provides a resin composition that simultaneously (1) supports high productivities, (2) is resistant to bleed out by the flame retardant present in the composition, (3) is resistant to migration of its components to another resin, (4) exhibits a high flame retardancy, and (5) exhibits high flexibility. The resin composition includes components (A) a polyphenylene ether, (B) a hydrogenated copolymer, (C) a styrene resin and/or olefin resin, and (D) a metal phosphinate, wherein the component (B) includes (B1) a polymer block principally comprising an aromatic vinyl monomer unit, and (B2) a hydrogenated copolymer block principally comprising an aromatic vinyl monomer unit and a conjugated diene monomer unit, and a content of the aromatic vinyl monomer unit in the (B2) is 20 to 95% by weight, and a content of the aromatic vinyl monomer unit in the (B) is 35 to 80% by weight.
    Type: Grant
    Filed: September 23, 2011
    Date of Patent: October 21, 2014
    Assignee: Asahi Kasei Chemicals Corporation
    Inventors: Yoshifumi Araki, Takashi Sato, Takahiro Hisasue
  • Patent number: 8722799
    Abstract: There is provided a thermoplastic elastomer composition having excellent flexibility, mechanical properties, scratch resistance, abrasion resistance, and low-temperature characteristics. A crosslinked thermoplastic elastomer composition comprising 5 to 70 parts by mass of (C) a hydrogenated product of a block copolymer having at least one conjugated diene monomer unit block and at least one vinyl aromatic monomer unit block, and 20 to 150 parts by mass of (D) an olefin-based resin, based on 100 parts by mass of the total of (A) an ethylene-?-olefin copolymer comprising an ethylene unit and an ?-olefin unit having 3 to 20 carbon atoms, and (B) a copolymer having at least one hydrogenated copolymer block mainly composed of a conjugated diene monomer unit and a vinyl aromatic monomer unit, wherein a mass ratio ((A)/(B)) of the (A) component and the (B) component is from 20/80 to 75/25.
    Type: Grant
    Filed: December 4, 2009
    Date of Patent: May 13, 2014
    Assignee: Asahi Kasei Chemicals Corporation
    Inventors: Yutaka Eguchi, Shinichi Shibayama, Yoshifumi Araki
  • Publication number: 20140121329
    Abstract: The present invention relates to a method for producing a hydrogenated conjugated diene copolymer including a polymerization step and a hydrogenation step, wherein in the polymerization step, a conjugated diene copolymer having a high vinyl bond amount of a conjugated diene block moiety and a narrow molecular weight distribution can be produced, and in the hydrogenation step, the rate of hydrogenation is high and productivity is excellent.
    Type: Application
    Filed: May 11, 2012
    Publication date: May 1, 2014
    Applicant: Asahi Kasei Chemicals Corporation
    Inventors: Yoshifumi Araki, Eiji Sasaya, Kenta Shibuya
  • Patent number: 8541504
    Abstract: Provided in this invention is an impact absorber composition comprising a copolymer containing an aromatic vinyl compound, wherein the peak of tan ? of the copolymer obtained from the measurement of the dynamic viscoelasticity is in the range of more than 0° C. to 20° C. or less, the value of tan ? is 0.4 or more in the whole temperature range of 5° C. to 15° C., and the value of tan ? at 15° C. is 0.5 or more.
    Type: Grant
    Filed: February 19, 2008
    Date of Patent: September 24, 2013
    Assignee: Asahi Kasei Chemicals Corporation
    Inventors: Yasuhiro Kusanose, Yoshifumi Araki
  • Publication number: 20130231430
    Abstract: The polyphenylene ether according to the present invention includes 5 to 20% by mass of a component having a molecular weight of 50,000 or more and 12 to 30% by mass of a component having a molecular weight of 8,000 or less. The resin composition according to the present invention includes the polyphenylene ether (a) and a hydrogenated block copolymer (b) prepared by hydrogenating a block copolymer including at least two polymer blocks A having a vinyl aromatic compound and at least one polymer block B having a conjugated diene compound, wherein the number average molecular weight (Mnb) of the hydrogenated block copolymer is 100,000 or less, and the number average molecular weight (MnbA) of at least one polymer block of the polymer blocks A is 8,000 or more.
    Type: Application
    Filed: October 13, 2010
    Publication date: September 5, 2013
    Applicant: ASAHI KASEI CHEMICALS CORPORATION
    Inventors: Shunichiro I, Yoshikuni Akiyama, Hiroshi Kamo, Yoshifumi Araki, Toru Yamaguchi, Tomohiro Kondo