Abstract: Molding compositions comprising a "terminally unsaturated"polyurethane, a copolymerizable vinyl or vinylidene compound and a rubbery-elastic polymer having a glass transition temperature of between -90.degree. and +10.degree. C. can be used for the preparation of molded articles having a considerably increased impact strength and a good heat distortion temperature, strength and rigidity.
Type:
Grant
Filed:
December 15, 1978
Date of Patent:
September 16, 1980
Assignee:
Bayer Aktiengesellschaft
Inventors:
Hannes von Harpe, Ludwig Bottenbruch, Bernd Peltzer, Leo Morbitzer, Helmut Korber, Hansjochen Schulz-Walz