Abstract: The strength of aromatic polyamide filaments spun at high speed downwardly through a non-coagulating fluid into a liquid coagulating bath and subsequently through a spin tube containing the freshly spun filaments and coagulating liquid is improved when the filaments are abruptly deflected away from the walls of the spin tube a distance of 0.025 to 0.15 times the inside diameter of the spin tube.