Abstract: A method for delignifying wood pulp and fiber is disclosed. The method comprises the steps of obtaining a wood pulp and exposing the wood pulp to a polyoxometalate of the formula [V.sub.l Mo.sub.m W.sub.n Nb.sub.o Ta.sub.p (TM).sub.q X.sub.r O.sub.s ].sup.x- where l is 0-18, m is . 0-40, n is 0-40, o is 0-10, p is 0-10, q is 0-9, r is 0-6, TM is a d-electron-containing transition metal ion, and X is a heteroatom, which is a p or d block element, where l+m+n+o+p.gtoreq.4, l+m+q>0 and s is sufficiently large that x>0. The exposure is under conditions wherein the polyoxometalate is reduced. In a preferable form of the invention, the method additionally comprises the step of reoxidizing the polyoxometalate.
Type:
Grant
Filed:
March 28, 1994
Date of Patent:
September 3, 1996
Assignees:
The United States of America as represented by the Secretary of Agriculture, Emory University
Inventors:
Ira A. Weinstock, Craig L. Hill, Rajai H. Atalla