Abstract: The invented method of cladding a metal component includes creating a frit mixture in a defined ratio; wetting the mixture by adding a wetting agent in a defined volume; agitating the wetted mixture; applying the agitated mixture to a metal component by one or more processes; de-wetting the metal component having the applied mixture by gradually heating the same to a temperature from approximately 250 degrees Fahrenheit (° F.) up to a high of approximately 450° F.; and, fusing the de-wetted metal component at a temperature of no more than 125% of a defined withstand temperature for the clad metal component. Invented compositions can include one or more of liquid and/or colloidal sodium, potassium and/or lithium silicate, clay and/or clays, a compound of hollow micro-spheres (e.g.
Abstract: The invented compositions for metal cladding of components in demanding applications can include one or more of liquid and/or colloidal sodium, potassium and/or lithium silicate, clay and/or clays, a compound of hollow micro-spheres (e.g. naturally occurring and nearly ubiquitous perlite and/or a synthetic hollow micro-sphere equivalent) and/or alumina or one or more flexible or malleable or resiliently deformable, impact-resistant materials such as plastomers, elastomers and/or other plastic, rubber, plastic-like or rubber-like materials; a wetting agent consisting of one or more of water or water and ethanol for fast drying under proper safety and venting conditions; and one or more surfactants and/or dispersants.