Patents Assigned to BHP Billiton SSM Development Pty Ltd.
  • Publication number: 20150152519
    Abstract: A process for the removal of ferric iron as hematite from a nickel solution containing ferric and ferrous ions including the steps of: raising the temperature of the nickel solution to between 90° C. and the boiling point of the solution at atmospheric pressure; raising the pH of the nickel solution to be between 2 and 3; and adding a hematite seed to facilitate hematite precipitation, wherein ferric ions are precipitated as hematite in a predominantly crystalline form.
    Type: Application
    Filed: June 21, 2013
    Publication date: June 4, 2015
    Applicant: BHP Billiton SSM Development Pty Ltd
    Inventors: Renato Antonio Loaiza Aguilar, Carolina Isabel Meneses Rodríguez, Ruben Rangel De Hoyos, Houyuan Liu
  • Patent number: 9028782
    Abstract: The present invention provides a method of separating nickel bearing sulphides from mined ores or concentrates of mined ores that contain talc particles is disclosed. The method comprises adjusting the Eh of a slurry of mined ores or concentrates of mined ores and making particles of nickel bearing sulphides less hydrophobic than talc particles and floating the nickel bearing sulphide particles from the slurry.
    Type: Grant
    Filed: January 9, 2009
    Date of Patent: May 12, 2015
    Assignee: BHP Billiton SSM Development Pty Ltd.
    Inventors: Geoffery David Senior, Brendan Pyke, Brian Judd
  • Publication number: 20150000466
    Abstract: A process for the production of a high grade nickel product including the steps of: a) providing at least one heap of a nickeliferous lateritic ore and leaching that heap with a suitable lixiviant, preferably sulfuric acid solution, to produce a nickel rich pregnant leach solution (PLS); b) subjecting the PLS to an impurity removal step to precipitate ferric iron, and preferably partially precipitate aluminium and chromium as hydroxides; and c) recovering a high grade nickel product from the PLS preferably by either nickel ion exchange, solvent extraction, electrowinning, conventional multi-stage neutralization, pyrohydrolysis or sulfidation.
    Type: Application
    Filed: February 13, 2013
    Publication date: January 1, 2015
    Applicant: BHP BILLITON SSM DEVELOPMENT PTY LTD
    Inventors: Houyuan Liu, Omar Yesid Caceres Hernandez, Renato Antonio Loaiza Aguilar, Carolina Isabel Meneses Rodriguez, Ruben Rangel De Hoyos, Illich Alvarez Mercado
  • Patent number: 8758479
    Abstract: A process is described for the recovery of nickel and/or cobalt from laterite or partially oxidized lateritic ores having a substantial proportion of the iron present in the ferrous state. The process includes providing a laterite or partially oxidized laterite ore wherein a substantial proportion of the iron present in the ore is in the ferrous state; acid leaching the ore to provide a product leach solution containing at least ferrous iron, nickel and cobalt together with acid soluble impurities; and recovering the nickel and cobalt from the product leach solution with a selective ion exchange resin in an ion exchange process leaving the ferrous iron and other acid soluble impurities in the raffinate.
    Type: Grant
    Filed: May 12, 2008
    Date of Patent: June 24, 2014
    Assignee: BHP Billiton SSM Development Pty Ltd
    Inventors: Omar Yesid Caceres Hernandez, Harald Muller, Graham Reynolds, Houyuan Liu
  • Patent number: 8753593
    Abstract: A method of separating nickel bearing sulphides from mined ores or concentrates of mined ores that contain talc is disclosed. The method comprises treating a slurry of mined ores or concentrates of mined ores in at least one flotation stage and in at least one cleaner circuit. The method further comprises sequenced re-grinding, as described herein, of particles in the slurry.
    Type: Grant
    Filed: January 9, 2009
    Date of Patent: June 17, 2014
    Assignee: BHP Billiton SSM Development Pty Ltd.
    Inventors: Geoffery David Senior, Brendan Pyke, Brian Judd
  • Patent number: 8734757
    Abstract: A process for producing a mineral concentrate product that at is at least a substantially odor-free product comprises any one or more than one of (a) organics removal by (i) treatment of a froth product slurry containing floated mineral particles to remove organic compounds from the mineral particles and/or (ii) thermal treatment, and (b) addition of chemicals to prevent residual organic compounds on mineral concentrates being converted to odorous compounds, particularly while the concentrates are being stock-piled or transported.
    Type: Grant
    Filed: April 6, 2009
    Date of Patent: May 27, 2014
    Assignee: BHP Billiton SSM Development Pty Ltd.
    Inventors: Chris du Plessis, Geoffery David Senior
  • Patent number: 8454723
    Abstract: A heap leach process for the recovery of nickel and/or cobalt from a laterite ore, said process including the steps of: a) providing one or more heaps of a nickeliferous laterite ore; b) leaching the ore in a heap leach step by applying acid to one or more heaps to provide a pregnant leach solution; c) neutralizing the pregnant leach solution with ground saprolite ore; and d) recovering the nickel and/or cobalt from the neutralized pregnant leach solution.
    Type: Grant
    Filed: June 16, 2009
    Date of Patent: June 4, 2013
    Assignee: BHP Billiton SSM Development Pty Ltd.
    Inventors: Houyuan Liu, Eric Girvan Roche
  • Patent number: 8366801
    Abstract: An atmospheric leach process for the recovery of nickel and cobalt from lateritic ores includes providing limonitic and saprolitic ore fractions of a laterite ore; separately slurrying the limonitic and saprolitic ore fractions to produce a limonitic ore slurry and a saprolitic ore slurry; separating any limonitic type minerals from the saprolitic ore slurry to produce a saprolitic feed slurry; milling or wet grinding the saprolitic feed slurry; leaching the limonitic ore slurry with concentrated sulfuric acid in a primary leach step; introducing the saprolitic feed slurry to the leach process in a secondary leach step by combining the saprolitic feed slurry with the leached limonite slurry following substantial completion of the primary leach step, and releasing sulfuric acid to assist in leaching the saprolite feed slurry.
    Type: Grant
    Filed: August 7, 2008
    Date of Patent: February 5, 2013
    Assignee: BHP Billiton SSM Development Pty Ltd.
    Inventors: Anthony Charles Chamberlain, Chad James Otto Czerny, Houyuan Liu, Harald Theowald Muller
  • Patent number: 8298501
    Abstract: A process for the recovery of a metal sulfide from a metal ion containing solution, including the steps of: a) providing a slurry containing seed panicles of said metal sulfide; h) adding a sulfide ion containing solution to said slurry to form an activated seed slurry; c) mixing said activated seed slurry with said metal ion containing solution to thereby form a metal sulfide precipitate; and d) recovering said metal sulfide precipitate.
    Type: Grant
    Filed: June 26, 2009
    Date of Patent: October 30, 2012
    Assignee: BHP Billiton SSM Development Pty Ltd.
    Inventor: Eric Girvan Roche
  • Patent number: 8268039
    Abstract: An atmospheric leaching process for the recovery of a nickel and cobalt from a lateritic ore includes (a) preparing a slurry of the lateritic ore with saline or hypersaline water having a total dissolved solids (TDS) content greater than 30 g/L; (b) leaching the slurry of the lateritic ore with sulfuric acid at atmospheric pressure, and (c) recovering nickel and cobalt from the resultant leachate.
    Type: Grant
    Filed: March 19, 2009
    Date of Patent: September 18, 2012
    Assignee: BHP Billiton SSM Development Pty Ltd.
    Inventors: Houyuan Liu, Graham Andrew Reynolds
  • Patent number: 8197575
    Abstract: A process for heap leaching a laterite that includes providing a primary and a secondary heap, with the primary heap comprising predominantly a nickel and cobalt containing sulfide or saprolitic type ore, and the secondary heap comprising predominantly a nickel and cobalt limonitic type ore; leaching the primary heap with a sulfuric acid solution to generate a solution that includes ferrous ions; and using the solution that includes the ferrous ion as the lixiviant to leach the secondary heap, to produce a pregnant leach solution that includes nickel, cobalt and manganese ions.
    Type: Grant
    Filed: December 24, 2008
    Date of Patent: June 12, 2012
    Assignee: BHP Billiton SSM Development Pty Ltd.
    Inventor: Adam Sean Moroney
  • Patent number: 7988938
    Abstract: A heap leach process for the recovery of nickel and cobalt from a lateritic ore, said process including the steps of leaching and/or agglomerating the ore with a lixiviant that includes ferrous ions, wherein the lixiviant is able to liberate cobalt from the cobalt containing minerals within the ore in preference to nickel, to produce a cobalt rich pregnant leach solution relatively free of nickel.
    Type: Grant
    Filed: December 24, 2008
    Date of Patent: August 2, 2011
    Assignee: BHP Billiton SSM Development Pty Ltd.
    Inventors: Eric Girvan Roche, Adam Sean Moroney, Houyuan Liu
  • Publication number: 20110123418
    Abstract: A process for the recovery of a metal sulfide from a metal ion containing solution, including the steps of: a) providing a slurry containing seed panicles of said metal sulfide; h) adding a sulfide ion containing solution to said slurry to form an activated seed slurry; c) mixing said activated seed slurry with said metal ion containing solution to thereby form a metal sulfide precipitate; and d) recovering said metal sulfide precipitate.
    Type: Application
    Filed: June 26, 2009
    Publication date: May 26, 2011
    Applicant: BHP BILLITON SSM DEVELOPMENT PTY LTD
    Inventor: Eric Girvan Roche
  • Patent number: 7935171
    Abstract: A process for producing a metallic nickel product with a low iron content, that includes: (i) providing an acidic product liquor; (ii) subjecting the acidic product liquor to an ion exchange process to absorb the nickel and part of the iron; (iii) eluting the nickel and iron to produce an eluate containing the nickel and iron. (iv) neutralising the eluate to leave an iron depleted eluate; (v) neutralising the iron depleted eluate to cause precipitation of nickel hydroxide containing low iron; (vi) calcining the nickel hydroxide to convert it to nickel oxide; (vii) subjecting the nickel oxide to direct smelting in the presence of a reductant to produce a molten nickel phase; and (viii) refining the molten nickel phase by oxidation to produce a metallic nickel product with low iron content.
    Type: Grant
    Filed: August 22, 2007
    Date of Patent: May 3, 2011
    Assignee: BHP Billiton SSM Development Pty Ltd.
    Inventors: Ivan Ratchev, Houyuan Liu, Alexey Duarte, Harald Theowald Muller
  • Publication number: 20100296988
    Abstract: A heap leach process for the recovery of nickel and cobalt from a lateritic ore, said process including the steps of leaching and/or agglomerating the ore with a lixiviant that includes ferrous ions, wherein the lixiviant is able to liberate cobalt from the cobalt containing minerals within the ore in preference to nickel, to produce a cobalt rich pregnant leach solution relatively free of nickel.
    Type: Application
    Filed: December 24, 2008
    Publication date: November 25, 2010
    Applicant: BHP BILLITON SSM DEVELOPMENT PTY LTD
    Inventors: Eric Girvan Roche, Adam Sean Moroney, Houyuan Liu
  • Publication number: 20100282024
    Abstract: A process for the recovery of nickel and/or cobalt from a lateritic ore by heap leaching, the process including the steps of: a) forming one or more heaps from a lateritic ore body wherein that lateritic ore body includes a blend of both limonitic and saprolitic type ores; b) leaching the one or more heaps with a leach solution; and c) recovering the nickel and/or cobalt from the resultant heap leachate.
    Type: Application
    Filed: September 12, 2008
    Publication date: November 11, 2010
    Applicant: BHP BILLITON SSM DEVELOPMENT PTY. LTD
    Inventors: Adam Sean Moroney, Omar Yesid Caceres Hernandez, Houyuan Liu
  • Publication number: 20100154593
    Abstract: A process for producing a metallic nickel product with a low iron content, including the steps of: (i) providing an acidic product liquor containing at least nickel and iron; (ii) subjecting said acidic product liquor to an ion exchange process wherein an ion exchange resin selectively absorbs said nickel and part of the iron from said product liquor; (iii) eluting the nickel and iron from said resin with an acidic solution to produce an eluate containing said nickel and iron. (iv) neutralising said eluate to a pH value in the range from 2.5 to 3.
    Type: Application
    Filed: August 22, 2007
    Publication date: June 24, 2010
    Applicant: BHP BILLITON SSM DEVELOPMENT PTY LTD