Abstract: A method of hard-facing a steel casting is described in which a hard-facing, which comprises a weld alloy matrix and a hard particulate substance, is attached to the casting by welding. In some embodiments the matrix can be of a similar composition to the casting, and in other embodiments the hard particulates can be rounded and/or substantially spherical, or of a substantially even size. A method is also described for hardening and tempering a steel casting after attaching the hard-facing to the casting by welding. After hard-facing the casting is hardened and tempered by heat treatment. In one embodiment the hard-faced casting is heat treated by heating to a temperature in excess of the austenitising temperature of the steel and then cooled by quenching in an aqueous solution, followed by tempering. In one embodiment the steel casting is tempered at a temperature in the range about 550° C. to about 700° C. prior to hard-facing the casting.