  • Patent number: 5902977
    Abstract: The present invention provides a process that employs both non-selective flotation and oxidative leaching of the resulting concentrates to recover an increased amount of copper from porphyry copper ores. The non-selective flotation step uses collectors and conditions, such as pH, that are conducive to the strong flotation of sulfide minerals generally. In the oxidative leach, the copper sulfide minerals in the concentrate fraction are oxidized to copper compounds, which are soluble in the leach solution. The oxidative leach includes the use of ammonia and sulfite under agitation leaching conditions to convert the copper sulfide minerals into ammonia soluble forms.
    Type: Grant
    Filed: July 14, 1997
    Date of Patent: May 11, 1999
    Assignee: COPROCO Development Corporation
    Inventor: Nathaniel Arbiter
  • Patent number: 5807479
    Abstract: The present invention provides a process that employs both non-selective flotation and oxidative leaching of the resulting concentrates to recover an increased amount of copper from porphyry copper ores. The non-selective flotation step uses collectors and conditions, such as pH, that are conducive to the strong flotation of sulfide minerals generally. In the oxidative leach, the copper sulfide minerals in the concentrate fraction are oxidized to copper compounds, which are soluble in the leach solution. The oxidative leach includes the use of ammonia and sulfite under agitation leaching conditions to convert the copper sulfide minerals into ammonia soluble forms.
    Type: Grant
    Filed: July 14, 1995
    Date of Patent: September 15, 1998
    Assignee: COPROCO Development Corporation
    Inventor: Nathaniel Arbiter
  • Patent number: 5795465
    Abstract: The present invention provides a process that employs both non-selective flotation and oxidative leaching of the resulting concentrates to recover an increased amount of copper from porphyry copper ores. The non-selective flotation step uses collectors and conditions, such as pH, that are conducive to the strong flotation of sulfide minerals generally. In the oxidative leach, the copper sulfide minerals in the concentrate fraction are oxidized to copper compounds, which are soluble in the leach solution. The oxidative leach includes the use of ammonia and sulfite under agitation leaching conditions to convert the copper sulfide minerals into ammonia soluble forms.
    Type: Grant
    Filed: July 15, 1994
    Date of Patent: August 18, 1998
    Assignee: Coproco Development Corporation
    Inventor: Nathaniel Arbiter