Abstract: Photoluminescent sand preferably includes play sand, photoluminescent pigment, a powdered binder and a curing agent. The play sand is preferably mixed with the photoluminescent pigment to form a photo sand mix. The photo sand mix is then mixed with the powered binder and curing agent to form the photoluminescent sand mix. The photoluminescent sand mix is allowed to cure for between 3-7 days to form the photoluminescent sand.
Abstract: Photoluminescent sand preferably includes play sand, photoluminescent pigment, a powdered binder and a curing agent. The play sand is preferably mixed with the photoluminescent pigment to form a photo sand mix. The photo sand mix is then mixed with the powered binder and curing agent to form the photoluminescent sand mix. The photoluminescent sand mix is allowed to cure for between 3-7 days to form the photoluminescent sand.
Abstract: A method of manufacturing a paving block with embedded photoluminescent material, comprising the steps of mixing sand, aggregate, water, and cement to form an uncured concrete mixture; mixing phosphorescent pigments, sand, cement, aggregate, and water to form an uncured phosphorescent mixture; providing a paving block mold; pouring the uncured concrete mixture into the paving block mold to fill the paving block mold; compressing the uncured concrete mixture in the paving block mold via a tamper head until the paving block mold is between 80% and 90% full; pouring the uncured phosphorescent mixture into the paving mold block to substantially fill the paving block mold; and compressing and vibrating the uncured concrete mixture and the uncured phosphorescent mixture in the paving mold block to generate an uncured paving block having a desired thickness and density.
Abstract: A paving block with improved illumination (luminescent paving block) preferably includes a concrete base layer and a photoluminescent layer. The photoluminescent layer is formed on top of the concrete base layer. The concrete base layer is preferably created by combining sand, aggregate, water, pigment and cement to form an uncured concrete mixture. The photoluminescent layer preferably includes very fine aggreagate, cement, water, pigment, sand and a polyester resin infused with a photoluminescent pigment or a silica-based glass material infused with photoluminescent pigment. Further, a light transmitting sealant may be placed over the photoluminescent material.
Type:
Application
Filed:
August 17, 2021
Publication date:
December 2, 2021
Applicant:
Glow Path Pavers, LLC
Inventors:
Alex Ketty, John Ketty, Jeremy P. Eckhous