Abstract: Coarsely crystalline aluminum oxide is provided which contains the following trace elements: V.sub.2 O.sub.5 > 0.005 percent by weight, P.sub.2 O.sub.5 > 0.005 percent by weight, Na.sub.2 O > 0.8 percent by weight.A method is provided for producing such an aluminum oxide by calcining aluminum hydroxide in the presence of at least one flouride and of vanadium salt.