Abstract: An environmentally friendly method for preparing zinc oxide (zincite) nanoparticle sol having more than 90% visible light transmission at 20 wt % solid; comprises of the neutralizing, under specific pH, an inorganic zinc salt with an inorganic alkali, both dissolved in ethylene glycol, and thermally aging the precipitates afterward.
Type:
Grant
Filed:
September 29, 2005
Date of Patent:
May 5, 2009
Assignee:
Headway Advanced Materials Co., Ltd
Inventors:
Anthony Shiaw-Tseh Chiang, Chih-Tsung Hsu, Ching-Ping Yang
Abstract: An environmentally friendly method for preparing zinc oxide (zincite) nanoparticle sol having more than 90% visible light transmission at 20 wt % solid; comprises of the neutralizing, under specific pH, an inorganic zinc salt with an inorganic alkali, both dissolved in ethylene glycol, and thermally aging the precipitates afterward.
Type:
Application
Filed:
September 29, 2005
Publication date:
October 5, 2006
Applicant:
Headway Advanced Materials Co., Ltd
Inventors:
Anthony Chiang, Chih-Tsung Hsu, Ching-Ping Yang