Abstract: A method for synthesizing a polybutylene adipate terephthalate-polylactic acid (PBAT-PLA) copolyester, the method including: uniformly blending a first prepolymer PBAT and a second prepolymer PLA to yield a mixture, 0putting the mixture in a vacuum reactor with a vacuum degree of between 5 and 100 pascal, heating the vacuum reactor to a temperature of between 100 and 110° C., and allowing to react for between 0.5 and 1 hr; stepwise increasing the temperature to be between 145 and 155° C. in between 1 and 2 hrs, and allowing to react for between 5 and 10 hrs, to yield a PBAT-PLA copolyester with a weight-average molecular weight of between 100000 and 250000. The method for synthesizing the PBAT-PLA copolyester is eco-friendly, non-toxic and cost-efficient.
Type:
Grant
Filed:
August 29, 2017
Date of Patent:
December 29, 2020
Assignee:
Henan Green Polymer Co., Ltd
Inventors:
Liuwen Ruan, Wanxin Li, Yongbin Tang, Xinyu He, Wenjun Yang, Bin Mao
Abstract: A method for synthesizing a polybutylene adipate terephthalate-polylactic acid (PBAT-PLA) copolyester, the method including: uniformly blending a first prepolymer PBAT and a second prepolymer PLA to yield a mixture, putting the mixture in a vacuum reactor with a vacuum degree of between 5 and 100 pascal, heating the vacuum reactor to a temperature of between 100 and 110° C., and allowing to react for between 0.5 and 1 hr; stepwise increasing the temperature to be between 145 and 155° C. in between 1 and 2 hrs, and allowing to react for between 5 and 10 hrs, to yield a PBAT-PLA copolyester with a weight-average molecular weight of between 100000 and 250000. The method for synthesizing the PBAT-PLA copolyester is eco-friendly, non-toxic and cost-efficient.
Type:
Application
Filed:
October 17, 2017
Publication date:
October 31, 2019
Applicants:
Henan Green Polymer Co., Ltd, Henan Green Polymer Co., Ltd
Inventors:
Liuwen Ruan, Wanxin Li, Yongbin Tang, Xinyu He, Wenjun Yang, Bin Mao