  • Patent number: 9050651
    Abstract: An ingot includes at least two metals selected from copper, tin, zinc and bismuth, wherein: (a) the ingot is a mechanical ingot, the at least two metals are 40-95 wt. % copper, 3-80 wt. % tin, 1-40 wt. % bismuth and/or 1-80 wt. % zinc, and other metals are present in a collective amount of 0-2 wt. %; or (b) the ingot is a cast ingot, the at least two metals are 40-80 wt. % copper, 3-80 wt. % tin, 1-40 wt. % bismuth and/or 1-80 wt. % zinc, and other metals are present in a collective amount of 0-2 wt. %, provided that when copper is present in the cast ingot in an amount greater than 69 wt. %, zinc is present in an amount less than 30 wt. %. Methods for preparing and casting the ingot are also disclosed, as is a system for casting a copper-bismuth alloy.
    Type: Grant
    Filed: June 14, 2011
    Date of Patent: June 9, 2015
    Assignee: Ingot Metal Company Limited
    Inventor: David Shore
  • Publication number: 20120321506
    Abstract: An ingot includes at least two metals selected from copper, tin, zinc and bismuth, wherein: (a) the ingot is a mechanical ingot, the at least two metals are 40-95 wt. % copper, 3-80 wt. % tin, 1-40 wt. % bismuth and/or 1-80 wt. % zinc, and other metals are present in a collective amount of 0-2 wt. %; or (b) the ingot is a cast ingot, the at least two metals are 40-80 wt. % copper, 3-80 wt. % tin, 1-40 wt. % bismuth and/or 1-80 wt. % zinc, and other metals are present in a collective amount of 0-2 wt. %, provided that when copper is present in the cast ingot in an amount greater than 69 wt. %, zinc is present in an amount less than 30 wt. %. Methods for preparing and casting the ingot are also disclosed, as is a system for casting a copper-bismuth alloy.
    Type: Application
    Filed: June 14, 2011
    Publication date: December 20, 2012
    Applicant: INGOT METAL COMPANY LIMITED
    Inventor: David SHORE