Abstract: Alkali metal hydroxide solutions containing substantial amounts of nitrate and nitrite which are contaminated by chromate are electrolytically converted to the corresponding hydroxides. The interference of the chromate with the normal electrolytic process is voided by adding bismuth ion to the solution and reversing the current direction at predetermined intervals.