Abstract: A method for the production of iron from an iron oxide-containing material includes contacting an iron oxide-containing material with a particle size distribution range with a ?90 of less than 2 mm, with a carbon-containing material with a particle size distribution range with a ?90 of less than 6 mm, in a commercial scale reactor at a temperature of between 900° C. and 1200° C. for a contact time sufficient to reduce the iron oxide to iron.