Abstract: The present invention discloses crystallized silicate-synthetic powder comprising a cordierite (2MgO.2Al2O3.5SiO2) crystalline phase, a mullite (3Al2O3.2SiO2) crystalline phase and a corundum (Al2O3) crystalline phase, and discloses a high-heat resistant porcelain body containing the above crystallized silicate-synthetic powder and formed by mixing the crystallized silicate-synthetic powder and kaolin mineral.
Abstract: The present invention discloses crystallized silicate-synthetic powder comprising a cordierite (2MgO.2Al2O3.5SiO2) crystalline phase, a mullite (3Al2O3.2SiO2) crystalline phase and a corundum (Al2O3) crystalline phase, and discloses a high-heat resistant porcelain body containing the above crystallized silicate-synthetic powder and formed by mixing the crystallized silicate-synthetic powder and kaolin mineral.
Abstract: The present invention discloses crystallized silicate-synthetic powder comprising a mullite (3Al2O3.2SiO2) crystalline phase, a anorthite (CaO.Al2O3.2SiO2) crystalline phase, and a corundum (Al2O3) crystalline phase, and discloses a high-strengthened porcelain body containing the above crystallized silicate-synthetic powder and formed by mixing the crystallized silicate-synthetic powder and kaolin mineral.
Abstract: The present invention discloses crystallized silicate-synthetic powder comprising a mullite (3Al2O3.2SiO2) crystalline phase, a anorthite (CaO.Al2O3.2SiO2) crystalline phase, and a corundum (Al2O3) crystalline phase, and discloses a high-strengthened porcelain body containing the above crystallized silicate-synthetic powder and formed by mixing the crystallized silicate-synthetic powder and kaolin mineral.