Abstract: A prefused basic flux composition comprising:______________________________________ SiO.sub.2 about 25 to about 35% Al.sub.2 O.sub.3 about 2 to about 6% TiO.sub.2 about 3 to about 7% CaF.sub.2 about 5 to about 11.25% CaO about 44 to about 52% MgO about 1 to about 10% MnO about 0.5 to about 5% Na.sub.2 O about 4.5 to about 8% K.sub.2 O about 0.5 to about 1.5% FeO 0 to about 2% ______________________________________And wherein the weight ratio of CaO to CaF.sub.2 is equal to or greater than about 4.
Type:
Grant
Filed:
December 13, 1976
Date of Patent:
January 3, 1978
Assignee:
La Soudure Electrique Autogene, Procedes Arcos, S.A.
Abstract: Flux for welding ordinary, semi-alloyed, alloyed or special steels with a high rate of efficiency and high rate of speed and containing a relatively high amount of Fe powder.
Type:
Grant
Filed:
April 13, 1976
Date of Patent:
July 19, 1977
Assignee:
La Soudure Electrique Autogene, Procedes Arcos, S.A.