Abstract: The mixture consists of at least one organic peroxide, at least one hydroquinone derivative of the general formulae I and/or II and/or III ##STR1## wherein R and R.sup.1, which may be identical or different, stand for H or t-alkyl, and X stands, for example, for C.sub.1-18 -alkylene, and a crosslinkage promoter, and permits the crosslinkage of polymers and at the same time extends the scorch time, which must be understood as the processing time.
Abstract: Optionally nucleo-substituted styrene polymers are crosslinked at temperatures above 110.degree. C. with combinations of crosslinkage promoters containing at least two polymerizable C--C double or C--C triple bonds in the molecule, and organic peroxides (with the exception of hydroperoxides, peracids, and ketone peroxides) having a 10 hour halflife temperature below 106.degree. C.
Abstract: A process is provided for crosslinking, foaming, or both of polymers at temperatures above 150.degree. C. using at least one azo ester and/or azo ether in combination with at least one crosslinking intensifier having at least two reactive carbon-carbon double or triple bonds.