Abstract: A novel method of sintering Si.sub.3 N.sub.4 shaped bodies which method comprises grinding Si.sub.3 N.sub.4 with the use of a grinding material down to a surface area magnitude of 10.5 to 35 m.sup.2 /g and an average particle size from 0.2 to 0.005 .mu.m, shaping the powder obtained, and sintering the compact under inert gas or nitrogen at a temperature from 1700.degree. to 1900.degree. C.
Type:
Grant
Filed:
January 27, 1988
Date of Patent:
March 13, 1990
Assignee:
Max-Planck-Gesellschaft zur Foedering der Wissenschaften e.V.
Inventors:
Nils Claussen, Jurgen Jahn, Gunter Petzow