Abstract: A die-casting aluminum base alloy consisting of, by weight %,Zn:10.about.25%, Si:6.about.10%,Cu:0.5.about.3.0%, Mn:0.1.about.0.5%,Mg:0.02.about.0.08%, Fe:less than 1.3%,and the rest of Al and unavoidable impurity.This alloy can be heat treated at low temperature from 260.degree. C. to 450.degree. C., at which steel parts inserted in this alloy will not deteriorate.This alloy has excellent mechanical strength, stress corrosion cracking resistance and wear resistance, and can be used for ball joints apparatus such as a stabilizer conrod for automobile.