Patents Assigned to Noritake Co., Limited
-
Publication number: 20120138872Abstract: A lead-free conductive compound for a solar cell electrode including: a conductive powder; a glass frit; and a vehicle; the glass fit includes at least one kind of lead-free glass including 10 to 29 (mol %) of Bi2O3, 15 to 30 (mol %) of ZnO, 0 to 20 (mol %) of SiO2, 20 to 33 (mol %) of B2O3, and a total sum 8 to 21 (mol %) of Li2O, Na2O and K2O which are contained in a ratio with respect to a whole of a glass compound in terms of oxides.Type: ApplicationFiled: May 28, 2010Publication date: June 7, 2012Applicant: NORITAKE CO., LIMITEDInventors: Yuko Suzuki, Takahiro Sugiyama, Yasushi Yoshino, Takehiro Nakao
-
Publication number: 20120112625Abstract: To provide a vacuum fluorescent display apparatus that can be expected to enhance lifespan characteristics of a red phosphor that does not contain Cd when driven in a voltage range of 30V or above. A vacuum fluorescent display apparatus comprising a filament cathode (10) and an anode (7); the filament cathode being arranged in a vacuum container, and used for releasing low-energy electrons; the anode having a phosphor (8) adhering thereto, and being struck by the low-energy electrons and thereby caused to emit light; wherein a structural body (9) is provided to a region in which the low-energy electrons released by the cathode can be controlled; the structural body having an electrically conductive or semi-conductive metal oxide formed at a portion that is bombarded by low-energy electrons.Type: ApplicationFiled: November 4, 2011Publication date: May 10, 2012Applicants: Noritake Co., Limited, Noritake Itron CorporationInventor: Koji Kato
-
Publication number: 20120012789Abstract: It is provided a fluorescent zirconia material including a fluorescent component and emitting fluorescence when excited with a light of a predetermined wavelength, the fluorescent component including a fluorescent material, the fluorescent material including at least one kind of Y2SiO5:Ce, Y2SiO5:Tb, (Y, Gd, Eu)BO3, Y2O3:Eu, YAG:Ce, ZnGa2O4:Zn and BaMgAl10O17:Eu and the fluorescent material being capable of emiting the fluorescence when subjected to firing treatment at temperatures ranging from 1300 to 1600(° C.) under oxidizing environments.Type: ApplicationFiled: March 17, 2010Publication date: January 19, 2012Applicant: NORITAKE CO., LIMITEDInventors: Yoshihisa Yamada, Yoshihisa Ito
-
Publication number: 20110309312Abstract: It is provided a paste composition for a solar cell electrode containing a conductive powder, a glass frit, and a vehicle, the glass frit being made of glass containing PbO, B2O3, and SiO2 at proportions within ranges of 46 to 57 (mol %), 1 to 7 (mol %), and 38 to 53 (mol %), respectively, in terms of oxide.Type: ApplicationFiled: January 28, 2010Publication date: December 22, 2011Applicant: NORITAKE CO., LIMITEDInventors: Takahiro Sugiyama, Atsushi Nagai, Ayumi Murakami
-
Publication number: 20110279425Abstract: The distance between filamentary cathodes and a phosphor on an anode substrate can be reduced by shortening the distance between the filamentary cathodes and a grid. To obtain high luminance without loss of display quality, the present invention provides a vacuum fluorescent display (1) with a driver IC, comprising a display unit (3) provided with a phosphor layer on an anode substrate (2), a plurality of filamentary cathodes (5), a grid (4), a driver IC (6), and a filament support (7) for shielding the IC and supporting an end part of the filamentary cathodes. The end part of the filamentary cathodes is fixed to one short side of the vacuum fluorescent display at a long side of the filament support. Depressions are provided to a surface of the filament support, or slits are provided to the filament support.Type: ApplicationFiled: May 13, 2011Publication date: November 17, 2011Applicants: NORITAKE CO., LIMITED, NORITAKE ITRON CORPORATIONInventor: Tadami Maeda
-
Patent number: 8038514Abstract: A milling tool includes a cylindrical base and a plurality of abrasive grain clusters. The cylindrical base is centrally formed with a through-hole, and has an annular surface extending around the through-hole, a peripheral surface extending perpendicularly to the annular surface, and an inclined or rounded surface connecting the annular and peripheral surfaces. The annular surface is formed with a circular recess groove coaxially with the through-hole for separating the annular surface into first and second planar areas that respectively are closer to and farther from the peripheral surface. The second planar area is higher than the first planar area. Abrasive grains are brazed on the annular surface. The abrasive grain clusters are brazed on the inclined surface at predetermined intervals, each cluster including a predetermined number of abrasive grains having substantially the same diameter, each cluster being positioned substantially on a circumference almost equidistant from one another.Type: GrantFiled: April 23, 2009Date of Patent: October 18, 2011Assignees: Noritake Super Abrasive Co., Ltd., Noritake Co., LimitedInventors: Yasuhiro Hidai, Naoki Toge, Shizuka Ishii
-
Patent number: 8021821Abstract: A photosensitive conductive paste for transferring including a metal powder, an inorganic material powder, a photosensitive resin and a polymerization initiator, and to be applied onto a surface of a transfer support, comprising an acrylic resin or a rosin-based resin.Type: GrantFiled: January 26, 2009Date of Patent: September 20, 2011Assignee: Noritake Co., LimitedInventors: Atsushi Nagai, Kazutaka Nakayama
-
Publication number: 20110215708Abstract: In order to provide a phosphor for a low-voltage electron beam and a vacuum fluorescent display apparatus in which the phosphor is used, a deposition layer is formed on a surface of a main body of a phosphor shown by the following chemical formula (1), the deposition layer being a plurality of oxide layers sequentially deposited on the surface of the phosphor main body. The phosphor for a low-voltage electron beam contains no cadmium, but has exceptional high-temperature exposure characteristics, as well as prolonged service life and higher brightness. Ca1-xSrxTiO3:Pr,M ??(1) where M is at least one element selected from Al, Ga, In, Mg, Zn, Li, Na, K, Gd, Y, La, Cs, and Rb; and 0?x?1.Type: ApplicationFiled: February 17, 2011Publication date: September 8, 2011Applicants: Noritake Itron Corporation, Noritake Co., LimitedInventor: Koji Kato
-
Publication number: 20110135906Abstract: A vitrified grinding stone includes: abrasive grains; an inorganic binder that binds the abrasive grains; and air-communicating pores that are formed between the abrasive grains and the inorganic binder, micro-capsules that each encapsulate a lubricant and each have a diameter that is smaller than that of the air-communicating pore, being fixed on an inner wall surface of each of the air-communicating pores by an adhesive.Type: ApplicationFiled: July 2, 2009Publication date: June 9, 2011Applicants: NORITAKE CO., LIMITED, NORITAKE SUPER ABRASIVE CO., LTD.Inventor: Akira Nagata
-
Patent number: 7938940Abstract: A support for an oxygen separation membrane element to support a dense and cylindrical electrolytic membrane having oxygen ion permeability, comprises a base axially extending and having a cylindrical surface extending axially, and a plurality of ribs formed on the cylindrical surface of the base, radially projecting and axially extending, for supporting the electrolytic membrane at their ends being radially distant from the cylindrical surface of the base.Type: GrantFiled: July 27, 2007Date of Patent: May 10, 2011Assignees: Noritake Co., Limited, Chubu Electric Power Co., Inc.Inventors: Akihiro Kawahara, Shigeo Nagaya, Hiroshi Seo
-
Patent number: 7884547Abstract: Lead-free acid-resistant glass composition includes 5-25% of SiO2, 4-30% of B2O3, 7-30% of ZnO, 15-70% of Bi2O3, 0-15% of Al2O3, 5-20% of BaO in weight percentage, and being substantially lead-free.Type: GrantFiled: February 1, 2008Date of Patent: February 8, 2011Assignee: Noritake Co., LimitedInventors: Yuko Kato, Makiko Imai
-
Publication number: 20100248936Abstract: It is provided a calcined ceramic body for dental use that is manufactured such that a formed body mainly containing zirconium oxide is worked in a degreasing process and in a calcining process, having a linear contraction coefficient upon full burning ranging from 19.0% to 22.0%.Type: ApplicationFiled: March 18, 2010Publication date: September 30, 2010Applicant: NORITAKE CO., LIMITEDInventors: Yoshihisa Yamada, Atsushi Matsumoto
-
Publication number: 20100194788Abstract: Luminance life can be enhanced in a vacuum fluorescent display that is driven according to a dynamic drive scheme and that uses a phosphor having remarkable luminance saturation. A drive method for a vacuum fluorescent display, having causing a phosphor layer formed on an anode to display under low-energy electron excitation by the dynamic driving, wherein the phosphor included in the phosphor layer is a phosphor in which the luminance increases when a pulse width is reduced under conditions in which the Du is kept the same in the dynamic driving, and in which, after a voltage is applied to the anode and the luminance of the phosphor is saturated, the time at which the luminance value decreases to 10% of the saturation luminance value following stoppage of the voltage application is 200 ?sec or more; and wherein the pulse width and pulse repetition period in the dynamic driving are made variable in the direction of maintaining the initial luminance of the phosphor as driving time elapses.Type: ApplicationFiled: January 26, 2010Publication date: August 5, 2010Applicants: NORITAKE ITRON CORPORATION, NORITAKE CO. LIMITEDInventors: Shigeki Kikuta, Kenji Nakanishi, Noboru Murata, Motohisa Isaka
-
Patent number: 7740773Abstract: The present invention provides a conductive composition and a conductive paste from which a conductive film having a high conductivity and a low thermal expansion coefficient can be formed. The thermal expansion coefficient of an island fixing type conductive layer 10 is compatible with that of a substrate 12. A cracking of the island fixing type conductive layer 10 or a crack in the substrate 12 due to a difference between these thermal expansion coefficients is suitably inhibited. The thermal expansion coefficient of the island fixing type conductive layer 10 is adjusted by ZWP contained in the range from 10 to 55 (wt %) as a low-expansion filler. Thus, compared with the case where other low-expansion filler is added, the conductivity degradation is inhibited. Accordingly, the island fixing type conductive layer 10 having a high conductivity and a high bonding strength is obtained.Type: GrantFiled: March 26, 2007Date of Patent: June 22, 2010Assignees: Noritake Co., Limited, Noritake Itron CorporationInventors: Motoki Iijima, Tatsuro Nishimura, Masayuki Nakanishi
-
Publication number: 20100128066Abstract: It is provided at a reasonable cost an image display method and image display apparatus having a small-sized display drive control circuits even in the case of many intensity levels. The plurality of bit strings constituting the indicative data D defining multiple intensity levels are divided into the first bit group including a plurality of bits and the second bit group including a plurality of bits except the bits included in the first bit group, and they are alternately supplied to the input terminals, predetermined light-emitting bodies 22 is lighted in an intensity level corresponding to the first bit group, in the first period K1 set in a luminous control period that is repeatedly assigned to the predetermined light-emitting bodies, and the predetermined light-emitting element 22 is lighted in a relatively finely-set intensity level corresponding to the second bit group, in the second period K2 set in a luminous control period.Type: ApplicationFiled: May 1, 2008Publication date: May 27, 2010Applicants: NORITAKE CO., LIMITED, NORITAKE ITRON CORPORATIONInventors: Noboru Murata, Toru Kohama, Masaaki Nakamura
-
Publication number: 20100038604Abstract: Nickel paste contains nickel powder, a resin binder and an organic solvent, wherein the nickel powder is a small amount sulfur nickel powder including less than 100 ppm sulfur. This provides the nickel paste that the change in viscosity due to sulfur included in the paste can be preferably restrained by using nickel powder including extremely small amount of sulfur. Limitation of sulfur to the extremely small amount causes superior stability, and then, since kinds of solvents and resin binders are not limited, the change in viscosity can be preferably restrained with using the solvent that is hard to cause the chemical attack on the green sheet as described above. Thus, nickel paste that is hard to cause the chemical attack and the change in viscosity can be provided.Type: ApplicationFiled: August 24, 2009Publication date: February 18, 2010Applicant: NORITAKE CO., LIMITEDInventor: Tsutomu SUGIYAMA
-
Publication number: 20090274524Abstract: A milling tool includes a cylindrical base and a plurality of abrasive grain clusters. The cylindrical base is centrally formed with a through-hole, and has an annular surface extending around the through-hole, a peripheral surface extending perpendicularly to the annular surface, and an inclined or rounded surface connecting the annular and peripheral surfaces. The annular surface is formed with a circular recess groove coaxially with the through-hole for separating the annular surface into first and second planar areas that respectively are closer to and farther from the peripheral surface. The second planar area is higher than the first planar area. Abrasive grains are brazed on the annular surface. The abrasive grain clusters are brazed on the inclined surface at predetermined intervals, each cluster including a predetermined number of abrasive grains having substantially the same diameter, each cluster being positioned substantially on a circumference almost equidistant from one another.Type: ApplicationFiled: April 23, 2009Publication date: November 5, 2009Applicants: NORITAKE SUPER ABRASIVES CO., LTD., NORITAKE CO., LIMITEDInventors: Yasuhiro Hidai, Naoki Toge, Shizuka Ishii
-
Patent number: 7588628Abstract: The present invention provides methods for making a microporous ceramic material using a metal silicon powder and including a reaction sintering process of the silicon. A material for forming a microporous ceramic material used in these methods includes a metal silicon powder, a silicon nitride powder and/or a silicon carbide powder, and if desired, a yttrium oxide powder and/or an aluminum oxide powder. These methods can make a microporous ceramic material that can be used preferably as a gas or liquid filter, a catalyst carrier or a support of a gas separation membrane.Type: GrantFiled: October 10, 2007Date of Patent: September 15, 2009Assignees: Noritake Co., Limited, Chubu Electric Power Co., Inc.Inventors: Yasunori Ando, Seiji Yamada, Hisatomi Taguchi, Yosuke Takahashi, Shigeo Nagaya, Kiyoshi Komura
-
Publication number: 20090197203Abstract: A photosensitive conductive paste for transferring including a metal powder, an inorganic material powder, a photosensitive resin and a polymerization initiator, and to be applied onto a surface of a transfer support, comprising an acrylic resin or a rosin-based resin.Type: ApplicationFiled: January 26, 2009Publication date: August 6, 2009Applicant: NORITAKE CO., LIMITEDInventors: Atsushi Nagai, Kazutaka Nakayama
-
Patent number: 7540802Abstract: A CMP pad conditioner is provided with a grinding part formed by fixing abrasive grains on a metal base by soldering, wherein the grinding part has a flat part near an inner periphery and an inclined part near an outer periphery, wherein abrasive grains having regular shapes are fixed to the flat part, and wherein abrasive grains having acute shapes are fixed to the inclined part.Type: GrantFiled: March 7, 2007Date of Patent: June 2, 2009Assignees: Noritake Co., Limited, Noritake Super Abrasive Co., Ltd.Inventors: Tetsuya Nonoshita, Naoki Toge