  • Patent number: 9574707
    Abstract: Disclosed is a method for manufacturing gas cylinders. The disclosed method for manufacturing gas cylinders comprises: a) a step of producing a liner using a liner blower machine; b) a step of applying an adhesive to the threads of the produced liner; c) a step of coupling a bushing to the threads of the liner; d) a step of leaving the liner having undergone step c) for 30 minutes to 2 hours at room temperature so as to naturally harden the adhesive; e) a liner-flaming step of heat-treating the outer surface of the liner with plasma; f) a step of coupling a shaft to the liner; g) a winding step of mixing multiple fiberglass strands with a resin and a hardening agent, and wrapping the mixture around the outer surface of the liner; h) a dry-hardening step of drying the cylinder made of the composite material and having undergone the winding step for 70 to 90 minutes at a temperature of 70° C. to 90° C.
    Type: Grant
    Filed: September 26, 2012
    Date of Patent: February 21, 2017
    Assignee: Norstar Composite Co., Ltd.
    Inventors: Ki Dong Kim, Gi Hun Kwon, Chang-Bae Lee
  • Publication number: 20150219277
    Abstract: Disclosed is a method for manufacturing gas cylinders. The disclosed method for manufacturing gas cylinders comprises: a) a step of producing a liner using a liner blower machine; b) a step of applying an adhesive to the threads of the produced liner; c) a step of coupling a bushing to the threads of the liner; d) a step of leaving the liner having undergone step c) for 30 minutes to 2 hours at room temperature so as to naturally harden the adhesive; e) a liner-flaming step of heat-treating the outer surface of the liner with plasma; f) a step of coupling a shaft to the liner; g) a winding step of mixing multiple fiberglass strands with a resin and a hardening agent, and wrapping the mixture around the outer surface of the liner; h) a dry-hardening step of drying the cylinder made of the composite material and having undergone the winding step for 70 to 90 minutes at a temperature of 70° C. to 90° C.
    Type: Application
    Filed: September 26, 2012
    Publication date: August 6, 2015
    Applicant: NORSTAR COMPOSITE CO., LTD
    Inventors: Ki Dong Kim, Gi Hun Kwon, Chang-Bae Lee