Abstract: High-quality machine parts, e.g. machine supports, are manufactured of concrete polymer on the basis of methacrylate monomer polymerizing at room temperature and of aggregates. The monomer used has a dynamic viscosity of less than 10 mPas (10 cP) preferably of 1-10 mPas (1-10 cP). The admixed starter system comprises an organic peroxide and an aromatic tertiary amine, the latter being dissolved in methacrylate monomer.
Abstract: High-quality machine parts, e.g. machine supports, are manufactured of concrete polymer on the basis of methacrylate monomer polymerizing at room temperature and of aggregates. The monomer used has a dynamic viscosity of less than 10 mPas 10cP, preferably of 1-10 mPas 10cP. The admixed starter system comprises an organic peroxide and an aromatic tertiary amine, the latter being dissolved in the methacrylate monomer.