Patents Assigned to Pou Chien Technology Co., Ltd.
  • Patent number: 8080589
    Abstract: A method for producing a bio-based polymeric shoe component includes: preparing a blend from a composition including 5˜50 weight parts of a modified starch, 50˜95 weight parts of an ethylene vinyl acetate copolymer, 5˜30 weight parts of a filler, 1˜50 weight parts of a polyolefin, 2.0˜8.0 weight parts of a foaming agent, 0.5˜3.0 weight parts of a foaming aid, 0.5˜2.0 weight parts of a lubricant, and 0.4˜1.2 weight parts of a crosslinking agent, the modified starch being obtained by hydrolyzing and esterifying a predetermined amount of a raw starch to form a hydrolyzed and esterified starch, followed by drying the hydrolyzed and esterified starch; processing the blend into a foamable product; and forming the foamable product into the shoe component.
    Type: Grant
    Filed: June 2, 2010
    Date of Patent: December 20, 2011
    Assignees: Pou Chien Technology Co., Ltd., Feng Chia University
    Inventors: Shu-Yii Wu, Shih-Chien Chu, Ting-Yu Lee, Ming-Lei Wang, Yan-Ting Shen, Ying-Ming Lu, Yu-Hsin Chu
  • Patent number: 8080596
    Abstract: A method for producing a biodegradable plastic material includes: hydrolyzing starch to form a hydrolyzed starch; esterifying the hydrolyzed starch to form a hydrolyzed and esterified starch; drying the hydrolyzed and esterified starch to obtain a dried modified starch; and mixing the dried modified starch with a plastic material, such as an EVA copolymer.
    Type: Grant
    Filed: January 8, 2009
    Date of Patent: December 20, 2011
    Assignees: Pou Chien Technology Co., Ltd., Feng Chia University
    Inventors: Shu-Yii Wu, Shih-Chien Chu, Ting-Yu Lee, Ming-Lei Wang, Chao-Wei Lin
  • Publication number: 20100237527
    Abstract: A method for producing a bio-based polymeric shoe component includes: preparing a blend from a composition including 5˜50 weight parts of a modified starch, 50˜95 weight parts of an ethylene vinyl acetate copolymer, 5˜30 weight parts of a filler, 1˜50 weight parts of a polyolefin, 2.0˜8.0 weight parts of a foaming agent, 0.5˜3.0 weight parts of a foaming aid, 0.5˜2.0 weight parts of a lubricant, and 0.4˜1.2 weight parts of a crosslinking agent, the modified starch being obtained by hydrolyzing and esterifying a predetermined amount of a raw starch to form a hydrolyzed and esterified starch, followed by drying the hydrolyzed and esterified starch; processing the blend into a foamable product; and forming the foamable product into the shoe component.
    Type: Application
    Filed: June 2, 2010
    Publication date: September 23, 2010
    Applicants: Feng Chia University, Pou Chien Technology Co., Ltd.
    Inventors: Shu-Yii WU, Shih-Chien Chu, Ting-Yu Lee, Ming-Lei Wang, Yan-Ting Shen, Ying-Ming Lu, Yu-Hsin Chu