Abstract: Filaments having a substantially increased inner surface, in particular porous filaments of filaments having a cracked, notched or nicked surface of thermoplsatic material are produced by subjecting filaments of thermoplastic material, preferably containing a pore-forming agent, to a heating medium at a temperature at least 100.degree., preferably 150.degree.C.