  • Patent number: 4464499
    Abstract: A wax which is suitable for use on low gloss resin exterior parts of an automobile, which comprises a microcrystalline wax having a melting point of 50.degree. to 100.degree. C. and/or a paraffin wax having a melting point of 40.degree. to 70.degree. C., a fatty acid amide, an isoparaffin and/or normal paraffin solvent having a boiling point of 100.degree. to 250.degree. C. and dimethylsilicone.
    Type: Grant
    Filed: May 19, 1983
    Date of Patent: August 7, 1984
    Assignees: Toyota Jidosha Kabushiki Kaisha, Sanko Chemical Co., Ltd.
    Inventors: Yoshiro Umemoto, Tsugumi Sanmiya, Mituo Kato
  • Patent number: 4272634
    Abstract: A process for the production of alcohols and/or aldehydes which comprises subjecting a toluene derivative having an ether linkage or linkages of the general formula: ##STR1## wherein RO is an ether grouping where R stands for a hydrocarbyl group with 1.about.20 carbon atoms which may carry an inert substituent or substituents and n stands for an integer of 1.about.2, to auto-oxidation with molecular oxygen in liquid phase to form the corresponding alcohol and/or aldehyde, characterized in that the reaction is carried out by using a lower saturated fatty acid and/or an anhydride thereof as solvent in the presence of a soluble cobalt salt and a bromine ion-supplying substance at a reaction temperature ranging from 30.degree. C. to 200.degree. C. in such manner that the conversion rate of the toluene derivative does not exceed 90%.
    Type: Grant
    Filed: December 11, 1979
    Date of Patent: June 9, 1981
    Assignees: Director-General of Agency of Industrial Science and Technology, Sanko Chemical Co., Ltd., Nippon Soda Co., Ltd.
    Inventor: Juichi Imamura
  • Patent number: 4220605
    Abstract: A process for the production of alcohols and/or aldehydes which comprises subjecting a toluene derivative having an ether linkage or linkages of the general formula: ##STR1## wherein RO is an ether grouping where R stands for a hydrocarbyl group with 1.about.20 carbon atoms which may carry an inert substituent or substituents and n stands for an integer of 1.about.2, to auto-oxidation with molecular oxygen in liquid phase to form the corresponding alcohol and/or aldehyde, characterized in that the reaction is carried out by using a lower saturated fatty acid and/or an anhydride thereof as solvent in the presence of a soluble cobalt salt and a bromine ion-supplying substance at a reaction temperature ranging from 30.degree. C. to 200.degree. C. in such manner that the conversion rate of the toluene derivative does not exceed 90%.
    Type: Grant
    Filed: December 23, 1977
    Date of Patent: September 2, 1980
    Assignees: Director General of Agency of Industrial Science and Technology, Sanko Chemical Co. Ltd., Nippon Soda Co. Ltd.
    Inventor: Juichi Imamura