Abstract: An admixture includes a first cementitious component, at least one unprocessed biomass component, calcium carbonate, an adhesive element, slag, amorphous silica, a water reducer, and fibers. The admixture is suitable for mixing with at least water to form a flowable material that cures to produce a hardened article. A method of producing a flowable material includes turning on a mixer and adding an unprocessed biomass component to a drum of the mixer. The unprocessed biomass component is sprayed with an adhesive element to form a first composition. Calcium carbonate is added to the first composition in the mixing chamber, to form a second composition. The second composition is mixed. A cementitious component is added to the mixed second composition in the mixing chamber, to form a third composition, which is mixed with water and calcium chloride to produce the flowable material. The flowable material cures to form the hardened material.
Type:
Application
Filed:
November 8, 2018
Publication date:
November 14, 2019
Applicant:
SBC Group LLC
Inventors:
James Paul Johnson, Robert Douglas Morris, Raymond W. Eley, JR., Christopher Klee Baird Morris
Abstract: An admixture includes a cementitious component, an unprocessed biomass component, calcium chloride, calcium carbonate, and an adhesive element. The admixture is suitable for mixing with water to form a flowable material that cures to produce a hardened material. A flowable material includes the admixture and water. A method of producing a flowable material includes turning on a mixer and adding an unprocessed biomass component to a drum of the mixer. The unprocessed biomass component is sprayed with an adhesive element to form a first composition. Calcium carbonate is added to the first composition in the mixing chamber, to form a second composition. The second composition is mixed. A cementitious component is added to the mixed second composition in the mixing chamber, to form a third composition, which is mixed with water and calcium chloride to produce the flowable material. The flowable material cures to form the hardened material.
Type:
Grant
Filed:
November 19, 2015
Date of Patent:
May 7, 2019
Assignee:
SBC Group LLC
Inventors:
Robert Douglas Morris, James Paul Johnson, Raymond W. Eley, Jr., Christopher Klee Baird Morris
Abstract: An admixture includes a cementitious component, an unprocessed biomass component, calcium chloride, calcium carbonate, and an adhesive element. The admixture is suitable for mixing with water to form a flowable material that cures to produce a hardened material. A flowable material includes the admixture and water. A method of producing a flowable material includes turning on a mixer and adding an unprocessed biomass component to a drum of the mixer. The unprocessed biomass component is sprayed with an adhesive element to form a first composition. Calcium carbonate is added to the first composition in the mixing chamber, to form a second composition. The second composition is mixed. A cementitious component is added to the mixed second composition in the mixing chamber, to form a third composition, which is mixed with water and calcium chloride to produce the flowable material. The flowable material cures to form the hardened material.
Type:
Application
Filed:
November 19, 2015
Publication date:
May 25, 2017
Applicant:
SBC GROUP LLC
Inventors:
Robert Douglas Morris, James Paul Johnson, Raymond W. Eley, JR., Christopher Klee Baird Morris